Variegated glossy blue M350 stoneware mug

Serial Number: AJ24143
Run/Test Number: P6723
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - GA6-B
Glaze Outside - GR6-M
Clay Body - M350
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 102 mm (4.0 in)
Depth at rim (including handle) - 134 mm (5.3 in)
Height - 124 mm (4.9 in)
Weight - 418 grams (14.7 oz)