Honey glazed cone 6 stoneware mug

Serial Number: AJ24313
Run/Test Number: L4453B
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - GA6-B
Clay Body - M340 Test
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 99 mm (3.9 in)
Depth at rim (including handle) - 133 mm (5.2 in)
Height - 129 mm (5.1 in)
Weight - 394 grams (13.9 oz)

Price:$40.00 (Not for sale, pieces being held for demo purposes)


PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy