Serial Number: AJ24040
Run/Test Number: P6845
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G1947U
Glaze Outside - G2571D
Clay Body - Polar Ice
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 88 mm (3.5 in)
Depth at rim (including handle) - 116 mm (4.6 in)
Height - 118 mm (4.6 in)
Weight - 334 grams (11.8 oz)
Price:$35.00 (Not for sale, pieces being held for demo purposes)