Rutile blue brown stoneware mug

Serial Number: AJ24168
Run/Test Number: 6723
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - GA6-B
Glaze Outside - GA6-C
Clay Body - M350
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 101 mm (4.0 in)
Depth at rim (including handle) - 135 mm (5.3 in)
Height - 119 mm (4.7 in)
Weight - 387 grams (13.6 oz)