Folded porcelain Sunshine mug

Serial Number: AJ24079
Run/Test Number: P6702
Technique: Hand-assembled, pour-glazed inside, waxed, liner-glazed inside, dip-glazed outside

Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G2934Y Yellow
Clay Body - M370
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 102 mm (4.0 in)
Depth at rim (including handle) - 123 mm (4.8 in)
Height - 104 mm (4.1 in)
Weight - 327 grams (11.5 oz)

Price:$25.00 (Not for sale, pieces being held for demo purposes)