White glazed speckled iron stoneware mug

Serial Number: AJ50023
Run/Test Number: L4168G6
Technique: Thrown, incised, dip-glazed

Temperature - Cone 10R
Glaze Inside - GR10-C
Glaze Outside - GR10-CW
Clay Body - H440
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 113 mm (4.4 in)
Depth at rim (including handle) - 136 mm (5.4 in)
Height - 110 mm (4.3 in)
Weight - 433 grams (15.3 oz)

Not for sale