Serial Number: AJ24322
Run/Test Number: P6902
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, bisque fired, dip glazed
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - GR10-C
Glaze Outside - G2571B
Engobe - L3954N
Clay Body - H450
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 100 mm (3.9 in)
Depth at rim (including handle) - 130 mm (5.1 in)
Height - 113 mm (4.4 in)
Weight - 424 grams (14.9 oz)
Price:$35.00 (Not for sale, pieces being held for demo purposes)