Bamboo tan incised H570 stoneware mug

Serial Number: AJ24139
Run/Test Number: P6699
Technique: Hand-rolled, embossed and assembled, liner-glazed inside, dip-glazed outside

Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G1947U
Glaze Outside - G2571A
Engobe - L3954N
Clay Body - H570
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 96 mm (3.8 in)
Depth at rim (including handle) - 123 mm (4.8 in)
Height - 102 mm (4.0 in)
Weight - 327 grams (11.5 oz)

Price:$40.00 (Not for sale, pieces being held for demo purposes)