Serial Number: AJ24027
Run/Test Number: P6816
Technique: Thrown, engobed, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G1947U
Glaze Outside - GR10-C
Engobe - L3954N
Clay Body - H550
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 102 mm (4.0 in)
Depth at rim (including handle) - 130 mm (5.1 in)
Height - 122 mm (4.8 in)
Weight - 433 grams (15.3 oz)
Price:$35.00 (Not for sale, pieces being held for demo purposes)