Rutile blue brown stoneware mug

Serial Number: AJ24078
Run/Test Number: P6823
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - L3500G+2Fe
Glaze Outside - GA6-C
Clay Body - M350
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 88 mm (3.5 in)
Depth at rim (including handle) - 117 mm (4.6 in)
Height - 109 mm (4.3 in)
Weight - 392 grams (13.8 oz)

Price:$35.00 (Not for sale, pieces being held for demo purposes)