Serial Number: AJ24416
Run/Test Number: P6731
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, bisque fired, dip glazed
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - GR10-C
Glaze Outside - GR10-C
Engobe - L3954N
Clay Body - H450
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 102 mm (4.0 in)
Depth at rim (including handle) - 139 mm (5.5 in)
Height - 122 mm (4.8 in)
Weight - 390 grams (13.7 oz)
Price:$45.00 (Not for sale, pieces being held for demo purposes)