Red and black porcelain mug

Serial Number: AJ24301
Run/Test Number: P6883
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G2926BL
Glaze Outside - G2934Y Red
Clay Body - P300
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 99 mm (3.9 in)
Depth at rim (including handle) - 128 mm (5.0 in)
Height - 122 mm (4.8 in)
Weight - 380 grams (13.4 oz)

Price:$50.00 (Not for sale, pieces being held for demo purposes)


PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy