Serial Number: AH24107
Run/Test Number: P6923
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G2934Y Black
Clay Body - Polar Ice
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 102 mm (4.0 in)
Depth at rim (including handle) - 130 mm (5.1 in)
Height - 106 mm (4.2 in)
Weight - 347 grams (12.2 oz)