Serial Number: AJ24362
Run/Test Number: P6947
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2926B white
Glaze Outside - GA6-B
Clay Body - M340
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 95 mm (3.7 in)
Depth at rim (including handle) - 129 mm (5.1 in)
Height - 113 mm (4.4 in)
Weight - 377 grams (13.3 oz)
Price:$35.00 (Not for sale, pieces being held for demo purposes)