Red Polar Ice mug

Serial Number: AJ50020
Run/Test Number: P7112
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G2926B Red
Clay Body - Polar Ice
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 90 mm (3.5 in)
Depth at rim (including handle) - 125 mm (4.9 in)
Height - 107 mm (4.2 in)
Weight - 335 grams (11.8 oz)