June 2026: We are continuing a major code rewrite. Please contact us if you find issues. Thank you.

Rutile blue red-brown stoneware mug

Serial Number: AJ24159
Run/Test Number: P6850
Technique: Hand-rolled, embossed and assembled, liner-glazed inside, dip-glazed outside

Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - L3500G+2Fe
Glaze Outside - GA6-C+2% iron oxide
Clay Body - M390
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 95 mm (3.7 in)
Depth at rim (including handle) - 130 mm (5.1 in)
Height - 102 mm (4.0 in)
Weight - 341 grams (12.0 oz)

Price:$35.00 (Not for sale, pieces being held for demo purposes)