Purple M340 mug

Serial Number: AJ50035
Run/Test Number: L3905J1C
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G2926B Purple
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 0 mm (0.0 in)
Depth at rim (including handle) - 0 mm (0.0 in)
Height - 0 mm (0.0 in)

Not for sale