Serial Number: AJ24151
Run/Test Number: BMix
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - GR10-C
Glaze Outside - G2571A
Engobe - L3954N
Clay Body - B-Mix 10
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 108 mm (4.3 in)
Depth at rim (including handle) - 136 mm (5.4 in)
Height - 122 mm (4.8 in)
Weight - 381 grams (13.4 oz)
Price:$30.00 (Not for sale, pieces being held for demo purposes)