Serial Number: AJ24102
Run/Test Number: P6770
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, bisque fired, dip glazed
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - GA6-C
Glaze Outside - GA6-C
Engobe - L3954B
Clay Body - M340
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 102 mm (4.0 in)
Depth at rim (including handle) - 133 mm (5.2 in)
Height - 121 mm (4.8 in)
Weight - 459 grams (16.2 oz)
Price:$35.00 (Not for sale, pieces being held for demo purposes)