Zero4 translucent fritware porcelain hash-tag mug

Serial Number: AJ24385
Run/Test Number: L3924J
Technique: Thrown, leather-hard under-glaze decorated, incised, 1650F bisque fired, dip-glazed

Firing Schedule - C04PLTP
Temperature - Cone 04
Glaze Inside - G3978C
Glaze Outside - G3879C
Clay Body - L3924J
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 89 mm (3.5 in)
Depth at rim (including handle) - 116 mm (4.6 in)
Height - 136 mm (5.4 in)
Weight - 350 grams (12.3 oz)