Black and white incised mug

Serial Number: AJ24328
Run/Test Number: P6901
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, bisque fired, dip glazed

Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - GR10-C
Glaze Outside - GR10-C MgO matte
Engobe - L3954N
Clay Body - H550
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 100 mm (3.9 in)
Depth at rim (including handle) - 134 mm (5.3 in)
Height - 115 mm (4.5 in)
Weight - 405 grams (14.3 oz)