These mugs are intended to demonstrate the techniques, recipes and materials I use as examples on this site. The intended audience is potters, hobbyists and manufacturers. Each mug described maintains its own permanent page here with detailed physical description as well as information on every detail of how it was made. Since each has links into many areas of this site that provide more detail, researching just one mug could take hours!
Serial Number: AJ24166
Run/Test Number: L4062A
Technique: Thrown, engobed inside and top outside, incised, dip-glazed.
Description: Needs refire
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G2571A
Glaze Outside - G2571A
Engobe - L3954N
Clay Body - H550
Foot Style - Bare unglazed
Width at rim (perpendicular to handle) - 114 mm (4.5 in)
Depth at rim (including handle) - 135 mm (5.3 in)
Height - 118 mm (4.6 in)