Serial Number: AJ24253
Run/Test Number: P6767
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - C5DHSC
Temperature - Cone 5
Glaze Inside - G2926B
Glaze Outside - G2926B purple
Clay Body - Polar Ice
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 91 mm (3.6 in)
Depth at rim (including handle) - 124 mm (4.9 in)
Height - 111 mm (4.4 in)
Not for sale