These mugs are intended to demonstrate the techniques, recipes and materials I use as examples on this site. The intended audience is potters, hobbyists and manufacturers. Each mug described maintains its own permanent page here with detailed physical description as well as information on every detail of how it was made. Since each has links into many areas of this site that provide more detail, researching just one mug could take hours!
Serial Number: AJ24170
Run/Test Number: P6626
Technique: Thrown, incised, dip-glazed
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G2926B
Clay Body - Polar Ice
Foot Style - Fluted foot ring
Width at rim (perpendicular to handle) - 99 mm (3.9 in)
Depth at rim (including handle) - 131 mm (5.2 in)
Height - 120 mm (4.7 in)