0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Rate | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition During Ceramic Firing | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | DTA Test | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | LAS Body | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | LOI-Adjust | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Interaction | Oxide Molecular Formula | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | TGA Test | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Molecular Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Slurry Up

The process of slurrying a clay body powder and dewatering it on a plastic slab or table.

Key phrases linking here: slurrying it up, slurry it up, slurrying up, slurried up, slurry up, slurry-up - Learn more

Details

In hobby ceramics and pottery, this expression is a verb referring to the preparation of a plastic clay body by weighing out the materials in the recipe, blending the powders, propeller-mixing them, and then dewatering the slurry (usually by pouring it onto a plaster table). Having the materials and equipment to prepare small amounts of clay bodies in this manner greatly enhances your ability to develop and test clay bodies (or even supply a production process if a plaster table is available).

Mixes that contain significant bentonite present special challenges when mixing with water. Some of these are so difficult that even high-speed propeller mixers cannot adequately remove agglomerates in slurries containing them. To deal with this it is very important that the powder batches be thoroughly mixed first before being added to the water (e.g. being vigorously shaken together in a plastic bag). This separates the bentonite particles, distributing them among the other materials in the recipe, thus preventing agglomerates from forming in the water. Mixes containing superfine materials like Veegum present another issue: They turn to jelly during mixing and can require much more water (perhaps double or even triple) in order to be fluid enough to move freely. If dewatering is needed it will obviously require much more time.

Watch for lumps, graininess and other signs of incomplete mixing in your slurries. Well-mixed ceramic slurries made from fine powders are creamy and silky smooth. If not then something is wrong. Blender mixing works extremely well for small batches and will create expectations when making larger batches.

Plastic bodies prepared in this manner require no deairing and no aging, the slurry mixing accomplishes both. If your plaster table is not waterlogged it can actually be faster to dewater slurries of higher water content, they spread out more thinly on the plaster and release their water more readily. Dewatering speed can also be improved by scraping up the clay, using a rubber rib, after the water sheen has disappeared, and turning it over and spreading it out.

Of course the term "slurry up" can also refer to mixing batches of casting slip, engobe, slip and even glaze.

Related Information

Testing your own native clays is easier than you think


Simple tests being done on a found clay

This picture has its own page with more detail, click here to see it.

Some simple equipment is all you need. You can do practical tests to characterize a local clay in your own studio or workshop (e.g. our SHAB test, DFAC test, SIEV test, LDW test). You need a gram scale (preferably accurate to 0.01g) and a set of callipers (check Amazon.com). Some metal sieves (search "Tyler Sieves" on Ebay). A stamp to mark samples with code and specimen numbers. A plaster table or slab. A propeller mixer. And, of course, a test kiln. And you need a place to put all the measurement data collected and learn from it (e.g. an account at insight-live.com).

Pouring the slurry on a plaster table to dewater it


This picture has its own page with more detail, click here to see it.

Pottery plaster is highly absorbent; it can remove the water from this thick slurry, made from a 5 kg powder mix, in an hour. Slurries of higher water content dewater much quicker; a 1 kg mix can be ready in minutes. This table weighs 400 lbs dry, but smaller ones are equally practical for smaller test batches. Plaster tables are much more practical in arid climates; it is dry here so one this size can supply enough clay for production of a potter. In wetter climates, ductwork can be installed within the plaster and air pressure can be used to dewater the table. If you need one of these, photos are linked to our plaster table article.

A recipe mixing area


This picture has its own page with more detail, click here to see it.

This was my Plainsman lab work area for mineral, frit, chemical, stain and metal oxide powders for developing glazes for customers and testing clay bodies and engobes. Not shown is the propeller mixer, perhaps the most important piece of equipment. And the plaster table for dewatering clay body slurries. Building up something like this, over time, is practical for any serious potter, many of these powders are inexpensive. Within minutes, I you can plan and enter a recipe into your Insight-live.com account, give it a code number, print it and weigh it out.

A must-have: Laboratory variable speed propeller mixer


This picture has its own page with more detail, click here to see it.

If you are at all serious about testing glazes and clay bodies, you need one of these. There are other methods, but nothing else comes close to this. It is the most valuable and frequently used tool in any ceramic bodies and glazes testing lab or classroom. This is the Lightnin brand, they are expensive but high quality. This is a 1/20 hp variable speed unit, it could be $4000 new! But you can get them used on ebay.com (the industrial mixers are most common, lab mixers are jealously guarded). This one uses a 7.9mm dia (5/16") shaft. We adapted a mount (to give it vertical adjustment) from small drill press.

Get a kitchen blender for mixing ceramic slurries


Freshly mixed clay slurry

This picture has its own page with more detail, click here to see it.

Blender mixing is invaluable in slurry preparation in small-scale ceramics and testing. It is quick and so effective that not only are particle surfaces wetted much better, but clay particles can actually be reduced in size (literally ground finer). Slurry rheology is also stabilized. For example, thixotropy can often be achieved naturally, without any additives. Materials that are otherwise impossible to mix into a slurry (e.g. bentonite, Veegum, CMC gum) or just difficult (e.g. titanium dioxide, tin oxide) are no problem. Even slurry-processed porcelains benefit, not only being more plastic, but firing to a more homogeneous surface and to greater density. Just visually, it is easy to see how much improved this MNP slurry is (a local clay with porcelaneous properties). It was mixed using our propeller mixer and seemed OK (on the left). But the improvement after only 20 seconds in the blender (right) is amazing.

A practical dust box may be better than a dust hood


A dust removal box

This picture has its own page with more detail, click here to see it.

An example of a custom-made dust collection hood in our repackaging and lab recipe mixing area. The slots along the front suck particles into the duct directly away from the operator's face. Suction comes from a centrifugal exhaust fan downstream where the pipe exits the building, it is driven by a 3/4hp motor (these fans are best at sucking, not blowing, so they need to be located at the exit). About 40 feet of 8-inch heating pipe connects from the hood to a fitting that expands to 12 inches going into the fan. The sliding damper above the hood enables stopping all airflow (to prevent heat loss during cold days). Notice it is located above the scale and heat sealer where most dust is generated during weighing and packaging.

Sanding the surface of a plaster table to keep it absorbent


This picture has its own page with more detail, click here to see it.

The water that a plaster table absorbs from clay slurries contains soluble salts. They penetrate into the plaster and then come back out to the surface as the water evaporates, forming a hard and less absorbent layer. Variable absorbency in a plaster surface can easily be observed as it is cleaned with a sponge and water. Fortunately, that layer is very thin and can be removed by sanding. Plaster is durable and can serve for decades using this technique. These durable fabric sand paper screens work exceptionally well because they can be used with water and to not blind. They are available in hardware stores and sold as drywall sand screens. We have seen 150, 120 and 80 grit (the latter is the one used here).

Links

Projects Evaluating a clay's suitability for use in pottery
Would you like to be able to use your own found-clays in your production? Follow me as we evaluate a mystery clay sample provided by a potter who wants to do this.
Projects Slurry Mixing and Dewatering Your Own Clay Body
Weigh out the ingredients, mix them using your propeller mixer and then dewater and fine-tune the stiffness on your plaster table.
Projects Make your own sieve shaker to process ceramic slurries
All you need is an inexpensive vibration motor from Amazon, a five-gallon pail, some metal and welding and 3D-printed collars to hold the sieve in place.
Glossary Blender Mixing
An ordinary kitchen blender does a better job of mixing a ceramic slurry than any industrial machine. It even reduces clay particle size and hyper ages it.
Articles Setting up a Clay Testing Program in Your Company or Studio
Set up a routine testing pipeline and start generating historical data that will enable your staff to understand your source materials and maintain, adjust and troubleshoot your clay body recipes.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy