0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Rate | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition During Ceramic Firing | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | DTA Test | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | LAS Body | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | LOI-Adjust | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Interaction | Oxide Molecular Formula | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | TGA Test | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Molecular Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Once-Fire

The practice of once-firing ceramics (no bisque) to produce fully glazed products. Considerable technical expertise and good testing are required to make it work. This is not a shortcut to skipping bisque firing.

Key phrases linking here: green glazing, green glazed, single-fire, once-fire - Learn more

Details

The practice of applying glazes to dried, rather than bisque-fired ware, and firing in one operation. Tradition is an important driver; some cultures have never used any other method. In industry (e.g. tile, sanitaryware, porcelain insulators), the advantage of the practice is saving energy and money. Understandably, many potters have or are considering single fire. But the difficulty of once firing is not to be underestimated, nor should it be considered a shortcut for skipping the bisque. Once-fire is a body-glaze-application-firing system.

Factors giving the greatest chance of success

A major challenge is to maintain the glaze slurry properties within an often narrow range of parameters (within which shrinkage can be tolerated, adherence is good, drying is efficient, and bonding is good). Each glaze must be tested thoroughly to discover this range and the methods needed to successfully apply and fire it. Often glaze recipes need to be adjusted (involving finding ways to increase the clay percentage while maintaining the chemistry). Common problems with the glaze itself include muddying of the body below, cracking and flaking during drying, crawling and blistering during firing, inadequate thickness and surface defects. Handling of the more fragile unfired ware (for application, cleaning, drying and setting) presents challenges. If ware is glazed at leather hard stage, extra drying times require extra floor space or special driers.

One caution: A high specific gravity does not automatically mean low water exposure during dipping. A strongly gelled slurry can deposit an excessively thick layer, carrying more total water onto the pot despite its high solids content. Deposit weight and application time should therefore be measured along with specific gravity.

Firing

A single firing is not simply an ordinary glaze firing containing unfired pots. Once firing brings the body-decomposition (bisque) and glaze-melting processes together in the same firing. Water vapour and gases from organics, clay minerals, carbonates, sulfates and other body or glaze materials must escape before the glaze seals the surface. If gas evolution continues after the glaze has begun melting, bubbles can be trapped or can break through too late for the surface to heal, producing microbubbles, pinholes, pits or blisters. Both the timing of gas evolution and the ability of the glaze melt to heal need to be considered.

Testing

A practical testing program should examine the merits of glazing leather-hard or bone dry, determine limits of wall thickness and construction methods, discover a glaze specific gravity and flow behaviour that work best, a suitable application method, limits of glaze thickness and layering, best preglaze preheat and drying time, best firing schedule and kiln atmosphere and factors that produce fired pinholing, blistering, crawling, or ware warping.

Handmade Tile

Manufacturers of industrial single-fired tile tightly control body preparation, pressing pressure, moisture content, glaze recipe (especially clay content) and application, drying and firing. But handmade tile makers are much less equipped to deal with the challenges for single firing. For bone dry tiles having a broad, thin, flat shape; water absorbed during glazing can itself curve them. But handmade shapes almost always have uneven wall thickness. Modern methods of 3D printing complex shaped tiles directly or using 3D tech to make intricate molds for casting them can produce even wall thicknesses. But clays suitable for casting are normally non-plastic and thus have much less ability to tolerate being rewetted without slaking or sagging; couple that with the fact that pieces are usually cast thin walled and glaze resetting issues are amplified. 3D printing clays are plastic, thus potentially better, and walls can be printed thicker. But shapes are often such that walls converge to create sections of double or triple thickness, a no-no for bone dry glazing.

For initial testing:

Related Information

Can bone-dry ware be glazed too thickly?

Yes! When the specific gravity is 1.7.


This picture has its own page with more detail, click here to see it.

In testing to determine the best specific gravity (SG) for this Darvan-deflocculated glaze slurry (G2926B), I arrived at what I thought would be great: 1.7. For 2.5kg of glaze powder only 1100g (1100ml) of water is needed, half the normal amount. And the slurry flows well. There appears to be enough water to form a good bond with the body. But a one-second dip of a bone dry piece produces twice the desired thickness, it dries too slowly and it is running. So, what should the SG be? I'll keep increasing the water until I can induce some thixotropy to hold it in place (using Epsom Salts), and it goes on thinner in a quick dip. If thixotropy is difficult, I’ll add 1% bentonite to increase particle surface area. And, I'll document the results at each step for future reference (in my Insight-Live account). Of course, these are going to need help drying, either by preheating the ware or putting the pieces in a drier.

From thrown to fired in 18 hours. How?


This picture has its own page with more detail, click here to see it.

Using a heat gun, it took 2-3 minutes to get this mug to soft leather-hard for trimming. It took 30 seconds to stiffen the handle for attachment afterward. I am now taking it to stiff leather-hard to prepare for glazing (left). Then I pour-glaze the inside and immediately push it lip-down into it to glaze the upper outside. I immediately gun it for a couple of minutes and then re-dip the outside bottom (up to the previous glaze boundary). Last, I gun it another 3 minutes and put it in the kiln for an hour at 250F for final water smoking. Finally, I fire 400F/hr to cone 6. The clay: Plainsman M370. The glaze: G3806C. The lesson: It is not the speed of drying; it is the evenness.

A once-fire mug vs. a bisque-fired mug


This picture has its own page with more detail, click here to see it.

The mug on the right was bisque-fired and then glazed, the one on the left was glazed in the green (dry) state using our standard meet-two-colors-at-the-rim glazing method. This method lends itself well to single fire glazing. Notice the glaze did not go on as thick on the once-fired piece (I should have used a slurry of higher specific gravity) and preheated the piece. In addition, there are a few pinholes, whereas the bisqued piece is flawless. Single-firing ware requires extra attention to firing, doing a bisque schedule first (to enable hydrates and carbon to escape) and then proceeding right into the glaze firing schedule.

Bisque-glazing vs. once-fire:

In medium temperature porcelain


This picture has its own page with more detail, click here to see it.

The mug on the left was bisque-fired and then glazed, the one on the right was glazed in the green (dry) state. The glazes are the same inside and out, but the porcelain one on the right is based on New Zealand kaolin (vs. American kaolin on the left). Three secrets for success for the one on the right were: It was glazed inside and out in two operations with a drying phase between; it was heated to about 150F before each application, and it was fired with a soaking period (at about 1900F) on the way up to top temperature (cone 6) to clear any gases generated by the body or glazes.

Single fire glazing done wrong


This picture has its own page with more detail, click here to see it.

The cone 6 porcelain mug on the left was successfully single-fire glazed by first pouring the inside (using a dipping glaze) and allowing that to dry thoroughly. The lip was then waxed, and the excess glaze that went over it was trimmed off. Finally, the outside was glazed by dipping the rim and then turning it over immediately and dipping down to the rim. The mug on the right was glazed on the inside and outside at the same time (by pouring, then dipping). As a result, it was over-whetted, and the body laminated within and bubbled during drying.

An alternative method: Mix it as a brushing glaze, apply one thinner coat at a time, drying each thoroughly before the next.

Links

Articles Creating a Non-Glaze Ceramic Slip or Engobe
It can be difficult to find an engobe that is drying and firing compatible with your body. It is better to understand, formulate and tune your own slip to your own body, glaze and process.
Glossary Rheology
In ceramics, this term refers to the flow and gel properties of a glaze or body suspension (made from water and mineral powders, with possible additives, deflocculants, modifiers).
Glossary Spray Glazing
In ceramic industry glazes are often sprayed, especially in sanitary ware. The technique is important.
Glossary Ceramic Glaze
Ceramic glazes are glasses that have been adjusted to work on and with the clay body they are applied to.
URLs https://www.luepottery.hwy.com.au/PDF/glaze%20spray.pdf
Glaze Spraying booklet by Roger Graham - Excellent reference
URLs https://digitalfire.com/4sight/datasheets/GlazeSprayingForCraftPotter.pdf
Glaze Spraying booklet by Rober Gramham #2
URLs https://www.instagram.com/reel/DVPM4MQCH-Y
Factory workers underglazing and glazing bone dry plates
The special dipping frame, application of colour as an underglaze, slurry rheology and very fast dip are the keys to making this possible.
URLs https://www.instagram.com/reel/DZUv9ZikQ-7
Factory worker finishing bone dry mugs
She uses a spinning sponge, fountain glazer and dip glazes the lip using a modified sieve
URLs https://www.instagram.com/reel/Db6gU0fCuMZ
Factory worker glazing bone-dry plates by spinning, sponging and dipping
The plates appear to be heated and the glaze is likely high-specific gravity because it dries incredibly fast.
URLs https://www.facebook.com/reel/1555758769633769
A factory worker dip-glazes translucent porcelain plates with her bare hands. Very fast!
She works at incredible speed, glazing one every two seconds. Without using dipping tongs. She applies a very thin layer of transparent glaze. While it appears very watery (low viscosity), it is likely high-solids and deflocculated to achieve extreme thixotropic behavior (fluid when moving, gelled when still). The speed of the dip, and fluid sweep while below the surface, ensure that all parts of the plate spend the same fraction of a second submerged, ensuring a uniform layer. Notice also that the plates on the split foam belt dry enough to stack within 10-15 seconds. What about the spot on the rim where she is holding it? Upon pulling the plate out, the glaze is still fluid enough to pool over it as a product of the way she releases it. Notice also that she picks them up with a glove, which means they may be hot (to speed drying). Finally, additions of surfactants and defoamers break the surface tension, enabling air bubbles to pop and smooth over quickly before the glaze dries. One final detail deserves repeating: This is translucent porcelain, maybe even bone china. That means the ware has been bisqued to zero porosity. Wow!

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy