0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Rate | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition During Ceramic Firing | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | DTA Test | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | LAS Body | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | LOI-Adjust | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Interaction | Oxide Molecular Formula | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | TGA Test | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Molecular Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Precipitation

Crystals or crystalline particles will often form over time in ceramic glaze slurries that contain slightly soluble materials.

Key phrases linking here: precipitation, precipitate - Learn more

Details

If a glaze slurry contains soluble or partially soluble raw materials or is made using hard water, then solids can precipitate over time forming hard lumps, crystals or a scum. At a minimum the solubility of many materials is enough to stain the water in a slurry (seen on the top after the powder has settled).

It seems logical that ceramic powdered materials, being ground up rock or glass (in the case of frits) would not be soluble. But this is not the case. Solubility is often a matter of chemistry. Certain frit chemistries, for example, are much more vulnerable to dissolution. This is because frits often need to push the boundaries of stability (therefore solubility) to deliver the desired chemistry (e.g. those lacking alumina). Frit production is not always precise, variations can lead to instability. Stains are also subject to solubility (for this reason some are acid washed).

Solubility of materials is often a simple product of increased surface area. For example, the solubility of feldspar or nepheline syenite rock is very low, but when ground into a powder its surface area is multiplied thousands or millions of times. This is enough to create noticeable solubility. Other materials are known to be contaminated by soluble salts. Gerstley borate, for example, gels glaze slurries, so obviously it is releasing ions into the suspension (its constituent minerals are also less stable than most other common ceramic materials). Ball clays likewise release scum as they dry (solubles are sourced from contaminants that get ground up with the clay itself, these are carried to the surface and precipitate there as brown scum as the water evaporates away). Manufactured materials like barium carbonate and lithium carbonate are partially soluble (this is just what they are).

Precipitation is not just a product of over saturation that occurs over time. It can also be a product of the interaction of various ions to be found in solution (which may well want to interact). Often it may appear that a particular material is guilty of precipitating in a specific glaze, however that same material may appear in another recipe where no precipitation occurs.

You can minimize precipitation and solubility in glazes by storing them in a cool place. And by making smaller batches and cycling them more often. Solubility of stains can affect the fired product (producing cloudiness on the surface of fired ware). In such cases it may be necessary to wash your stains before use (in vinegar for example).

Related Information

Can frits be partially soluble? Yes, and here is what that means.


This picture has its own page with more detail, click here to see it.

These 1 mm-sized crystals were found precipitated in a couple of gallons of glaze containing 85% Ferro Frit 3195. They are cubical, hard and insoluble. Why and how to do they form? Many frits are slightly soluble, the degree to which they are is related to the length of time the glaze is in storage, the temperature, the electrolytes and solubles in the water, interactions with other material particles present and the diligence of the manufacturer in mixing, correctly achieving the target chemistry and firing. The solutes interact or saturate to form insoluble species that crystallize and precipitate out as you see here. These crystals can be a wide range of shapes and sizes and come from leaded and unleaded frits. In industry this issue is not generally a problem because glazes are used soon after being made.

A glaze slurry precipitates flakes


This picture has its own page with more detail, click here to see it.

These flakes have been screened from a highly-fritted boron glaze mixed using hard water and stored for a year. They formed as a film across the top of the settled surface and on the walls of the bucket. Frits are stoichiometric, they should not dissollve, but they do. Perhaps this is evidence that frit makers are unable to precisely control production parameters.

G2926B glaze can precipitate crystals like this


This picture has its own page with more detail, click here to see it.

These crystals were found in a months-old bucket (about 2 gallons). These can appear even quicker, depending on factors like temperature, electrolytes in your water or solubility in the materials (evens frits can be slightly soluble). The glaze slurry should be screened periodically (or immediately if you note the particles when glazing a piece). This is an 80 mesh sieve. Note the brush, using one of these gets the glaze through the screen much quicker than using a rubber spatula. The loss of material on the screen is tiny and inconsequential to the glaze. But it is crucial because these particles do not melt at cone 6, they will certainly mar the fired glaze surface if undetected.

Precipitated crystals from a glaze having 60% lead bisilicate frit


This picture has its own page with more detail, click here to see it.

It also contains less than 10% borax frit and some Cornwall stone.

Soluble ingredients in glazes always precipitate as angular crystals. Right?


This picture has its own page with more detail, click here to see it.

Wrong. These tiny spheres (actually they are not so tiny) form over time as a precipitate in a glaze having a high concentration of a boron frit and mixed in hard water. This may be an example of how interactions can affect the degree to which materials dissolve in water (in this case the electrolyte in the water could be a trigger). These are likely ooids.

Here is what happens if you do not sieve your glazes when needed


This picture has its own page with more detail, click here to see it.

This is a cone 6 transparent base glaze. It contains frit, silica, kaolin, wollastonite. Almost all glazes have materials that are slightly soluble and over time these can form scale on the sides of the bucket or even precipitate particles into the slurry. The defects here are those scales. Before dipping a production piece in any glaze that has been in storage it is a good idea to assess it first to see if it needs to be sieved.

Add 5% calcium carbonate to a tenmoku. What happens?


This picture has its own page with more detail, click here to see it.

In the glaze on the left (90% Ravenscrag Slip and 10% iron oxide) the iron is saturating the melt crystallizing out during cooling. GR10-K1, on the right, is the same glaze but with 5% added calcium carbonate. This addition is enough to keep most of the iron in solution through cooling, so it contributes to the super-gloss deep tenmoku effect instead of precipitating out.

Unusual crystal precipitate in frit+lithium glaze


This picture has its own page with more detail, click here to see it.

In this case, lithium carbonate was added to the G1214Z1 cone 6 matte glaze base. These formed sometime later.

Links

Glossary Water Solubility
The water solubility of ceramic materials is an important consideration to their usability in the process. Glazes are suspensions of insert powders, solubles present problems to this system.
Glossary Agglomeration
The fine mineral, oxide and clay particles used in ceramics often aglommerate during storage or even in the latter stages of production. These must be broken down later.
URLs https://en.wikipedia.org/wiki/Precipitation_(chemistry)
Precipitation at Wikipedia
URLs https://en.wikipedia.org/wiki/Ooid
Ooids in Glazes

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy