0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Rate | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition During Ceramic Firing | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | DTA Test | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | LAS Body | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | LOI-Adjust | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Interaction | Oxide Molecular Formula | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | TGA Test | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Molecular Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Shino Glazes

Traditional Japanese high feldspar glazes having cream to orange color flashing or blushing. Potters today seek to emulate the Shino appearance using a wide range of recipes.

Key phrases linking here: shino glazes, shino - Learn more

Details

Shino glazed small bowl from Japan



Shino glazes were developed in Japan and their aesthetics are covered on many other websites and books. But they are art pieces, described by artists, using the language of art. Although the term Shino has become very broad in recent years let us restrict this to the visuals of the "pearly white breaking to orange" and the carbon trapping (which leaves random dark, shadowy areas in the glaze). Of course, there is also a mystique surrounding the bubbling and crawling effects of many of the most loved pieces. While we might consider these as defects, traditionally they were considered decorative and pleasing. However, this page is about understanding the chemistry and the other mechanisms of color and surface development with the objective of making consistent and functional pieces.

Originally Shinos were a two-part mix of about 70-80% high-alumina, high-sodium feldspar and 20-30% clay. They were used on stoneware and wood-fired in reduction. Applied thickly they gave a pearly white, when thinner a red or orange. While it is claimed that the combination of high sodium and alumina produce that orange color, it seems that would not be possible without iron. In fact, it is the chemistry of the glaze that hosts the color, amplifying the color of small amounts of iron in the clay (within the glaze or in the body itself) to produce the orange color.

Potters doing utilitarian pieces with the Shino effect today often need a more glossy, functional finish (instead of the traditional crawled matte with blisters and pinholes!). They also want something that can be put into an existing firing with other ware (e.g. cone 10 reduction). Recipes found online can have up to a dozen ingredients. However given the simplicity of the original, it would appear that needlessly complex recipes are unnecessary (likely a product of the blending of other multiple recipes). It is best to approach your search armed with a little background knowledge. In fact, you might find a better approach is to simply propose a recipe, based on the conclusions drawn below, and try it (albeit without a wood kiln and all the firing magic it did to create the original effects). Let's do that.

Recipes trying to stay true to the original Shino spirit seem to follow these general guidelines:

-A high percentage of nepheline syenite producing a very high Al2O3 level in the flux unity formula, usually higher than 1.0 going even to 2.0 (you will see this number calculated by entering the recipe into your account at insight-live.com). No other type of common glaze recipe used in ceramics has even close to this amount of Al2O3.

-No added silica (and an Al2O3:SiO2 ratio usually well below 5:1).

-Enough clay to suspend the glaze (these add even more Al2O3 than what is in the Nepheline). Kaolins and ball clays are used. The more alumina that can be sourced from the feldspar the more feasible it is to employ ball clay rather than kaolin (ball clay has lower Al2O3).

-Low CaO (it inhibits the orange color).

-Soluble sources of sodium (e.g. soda ash, salt) are often employed. These are thus not being added to simply boost the Na2O content, since they will migrate and concentrate at the surface during drying. However that is likely the whole point, given another practice: Mixing up a super-saturated solution of soda ash and hot water and spraying it onto a glaze, carbon trapping occurs in the sprayed area (assuming the firing promotes carbon trapping).

-A small amount of iron-bearing clay.

-Often small to significant amounts of tin oxide (up to 10%, exceptionally expensive!). Why? Maybe it is there as a catalyst to develop the color of the iron. There is also a possibility the tin is opacifying to crow-bar the opaque cream effect in oxidation firing (especially where more powerful melters are being employed, ones which will make the glaze more transparent).

-Super melters that source boron (from frits or Gerstley Borate), lithium (from Spodumene and lithium carbonate) and even zinc are employed in some recipes. These could be there to melt early and seal the surface. However some control is needed or the thick, opaque and pearly nature of the surface would be lost. These alternate fluxes also have another key effect: low thermal expansion. If they are employed at the cost of sodium, significant reductions in thermal expansion of the glaze would result (reducing crazing).

There are recipes claiming to be Shino that deviate completely from every guideline already given: having high silica:alumina ratios, low sodium, high iron or high CaO. As noted, some employ ridiculous percentages of tin oxide. If you are new to Shinos it might be better to stick with the simpler recipes and focus more on the techniques and the firing to achieve the effect. If you enter the recipes in your account at insight-live.com you can see the chemistry (and compare many side-by-side, especially on a widescreen monitor). As noted, look for the low Al2O3:SiO2 ratio, Al2O3 above 1.0, low CaO, high Na2O. Optionally some iron-bearing clay and maybe some tin oxide.

Some authors discuss the "orange flashing" effect of Shinos (as if the orange effect is on the surface, overlaying the cream background). However, I have not seen this. The Shino visual seems much more basic: Orange where thin, cream where thick. However, given the absence of an iron wash below the Shino (which would obviously produce color where the glaze is thin), there is some mystery to how the color appears to develop at the body:glaze interface (showing through where the glaze is thinner). This happens even when the body is white. How?

As noted, Shinos traditionally crawl, craze, pinhole and carbon trap. These are natural products of the chemistry and firing: pinholing and crawling because the melt is viscous, crazing because of the high sodium and carbon trapping because of early melting and heavy reduction. Carbon trapping will obviously happen more if reduction is started earlier (e.g. cone 012), of course, other ware in the kiln needs to be able to tolerate this. And trapping will be better if the reduction is heavier. Some claim that lower amounts of Al2O3 in the formula (below 1.0) better trap the carbon. Yet carbon trap recipes are out there with much more alumina. Of course, using low-carbon bodies or bisquing hot will eliminate this problem (if you want to).

One of my efforts at Shino (see below)



Crawling can be minimized if you want to. Glazes with 30% clay, especially if that clay is ball clay, will shrink excessively during drying. The crack lines will then crawl during firing (especially since the Shino chemistry is high in alumina and therefore has a low melt viscosity). Simply calcining part of the clay will reduce the problem. Aim for about 15-25% raw clay (the rest calcined).

Pinholing can be reduced by using a finer quality body (that does not generate as many gases) or by applying the glaze thinner. Or by compromising the chemistry a little to get better melt fluidity. Or, as noted above, bisquing hotter.

Crazing is the most difficult issue (crazing is not desirable or even acceptable in functional ware being sold to the public). Shino glazes have high thermal expansion (although some recipes certainly are lower than others). Insight-live displays the calculated thermal expansion (these will likely calculate to the highest numbers you have ever seen!). As already noted above, a strategy to lower the expansion is to trade some of the sodium for low-expansion fluxes like lithia, zinc or boron. Another option is to use a high-silica body. It is possible to make vitreous bodies with up to 40% silica at cone 10. Such bodies are also useful for crystalline glazes (which also craze badly).

So what glaze should we propose for a cone 10 reduction recipe, given the above? Here is my idea (code G3840 in my Insight-Live account):

Nepheline Syenite 50
Spodumene 15
Kaolin 20
Soda Ash 10
Redart 5

Related Information

Closeup of Shino glazed small bowl from Japan


This picture has its own page with more detail, click here to see it.

Clay is vitreous and heavily grogged. But it is white burning. Notice the orange color is developing at the glaze/body interface and shows where the glaze is thin. This is glossier than what one would normally expect a Shino to be.

Heavily speckled reduction fired porcelain Shino bowl by Glenn Lewis


This picture has its own page with more detail, click here to see it.

This effect was created by wedging 10 mesh ironstone concretions into the soft porcelain.

Shino bowl made by Joshua Miller


This picture has its own page with more detail, click here to see it.

White body. Double fired, first to cone 11 (reduced from 1800F up as for copper reds). A thin second layer of the Shino glaze was applied and a second slow-climb firing was done to cone 05, this produced the metallic effect. This is a Malcom Davis glaze (with Redart). Joshua Miller, the creator of this piece, mentors under his father, Victor Miller.

Closeup of unglazed surface of small Shigaraki bowl


This picture has its own page with more detail, click here to see it.

This is the unglazed surface. Very heavily grogged, very large grog particles.

Closeup of unglazed surface of small Bizen bowl


This picture has its own page with more detail, click here to see it.

The fired clay is vitreous and lightly grogged (large particles).

G3840 Shino on Grolleg/New Zealand kaolin porcelain at cone 10R


This picture has its own page with more detail, click here to see it.

The color is developing despite the fact that very little iron is available from the body. I have glazed the inside of this mug with a durable liner glaze to make it functional. The porcelain contains more than 30% silica but the Shino is still crazing on it.

Calculating the recipe of a cone 10R Shino glaze


Two small brown, matte shino bowls

This picture has its own page with more detail, click here to see it.

The wax resist brushstrokes (done right after glazing) are clearly defined indicating that soda migration to the surface during drying is an important mechanism of the effect. Some carbon trapping is also visible on the lower section of the larger bowl (and other pieces in other places in the kiln). The glaze has been applied fairly thinly so no whiter areas are visible. This was part of a project I did to understand, not what Shino glazes look like, but what they are. Chemically. The code for the project was G3840.

Links

Glossary Carbon trap glazes
A type of ceramc glaze.
Glossary Carbon Burnout
Ceramic materials, especially clays, often contain carbon and organic compounds. When they are fired in a kiln, these must burn out, often producing complications.
Glossary Calcination
Calcining is simply firing a ceramic material to create a powder of new physical properties. Often it is done to kill the plasticity or burn away the hydrates, carbonates, sulfates of a clay or refractory material.
Glossary Ceramic Glaze
Ceramic glazes are glasses that have been adjusted to work on and with the clay body they are applied to.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy