0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Rate | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition During Ceramic Firing | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | DTA Test | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | LAS Body | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | LOI-Adjust | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Interaction | Oxide Molecular Formula | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | TGA Test | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Molecular Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Artware

Artware, to potters and hobbyists, is pottery made from white-burning clays fired at low temperatures with brightly coloured glazes and decorated using decals, underglazes, lustres, etc.

Key phrases linking here: talc body, art ware, artware - Learn more

Details

News Fall 2021: The hobby casting and artware markets have been turned upside down in North America. White Texas talc is is now surrounded by a climate of legal chill (for potential asbestos content). Suppliers are working on the problem and it appears dolomite can be used as a substitute without loss of whiteness. And dolomite has no health issues. Bodies will have a lower firing shrinkage and higher porosity.

When you buy a low temperature white burning body from a ceramic supplier you are buying what the industry calls a 'talc body'. Talc bodies are basically 50% ball clay and 50% talc. The ball clay imparts great dry strength for handling and the talc improves the casting, drying and glaze fit properties. The use of this type of body started in the hobby-casting industry and it became a standard on which the prepared glaze industry could rely. Bodies are very stable when fired to cone 05-06, they do not warp, even on thin pieces. And they often fire amazingly white compared to stonewares, thus bright colored glazes work well on them. This enables artists to almost completely forget about technical issues of casting, glazing and firing and focus purely on aesthetics - thus the term "Artware".

Manufacturers of modelling, throwing and sculpture bodies of this type could be adapted to plastic forming by simply adding a little bentonite to improve plasticity. Such bodies have among the best throwing properties of any clay available. The beauty of this adaptation is that the whole world of prepared glazes is then available to potters and sculptors.

The Down Side

Firing and fired properties had to be compromised to get the easy working properties. Firing is done at cone 06-04, pieces are weak, you can rip some apart with your bare hands.

These bodies are only lightly sintered, they fire white simply because there is no glass development taking place, no 'glue' is forming to cement the matrix together or bring out the color of the iron.

Glaze fit: Glaze is just not 'glued on' very well. Therefore crazing and shivering will occur with much smaller thermal expansion mismatches between body and glaze compared to stoneware.

Food Safety: Low fire glazes are potentially more soluble and prone to leaching than stoneware. Most glazes are high in frit so they inherit the food safety of the frits used. However there are many ways to combine frits and additives to make glazes unsafe, unconventional recipes, especially bright colors and crystallization effects, need thorough testing to assure food safety.

Porosity: Low fire bodies are porous, they soak up water like a sponge. If a piece stays wet it can breed bacteria. If the water gets between two glazed walls it can explode a piece when it turns to steam during heating.

Low fire talc bodies are a bit of a king-with-no-clothes situation, they pretend to be ceramic with fancy glossy glazes but underneath they are porous and weak and unceramic.

The Materials

Talc is used in low fire hobby bodies to increase the thermal expansion, without it it is very difficult to create glazes that do not craze. Talc is also the filler, diluting the plasticity and reducing the drying shrinkage of the ball clay. Very few talcs are white enough (most fire yellowish or even brownish), in North America only Texas talcs are suitable.

Ball clay imparts plasticity to clay bodies. Ball clays are much too plastic to use alone. Ball clays are dirty (high in iron) compared to kaolins, it is normal to seek out the whitest ball clays available, especially those that have low soluble salts content.

Bentonites are ball clays on steroids! They add a lot of plasticity in small percentages. Bentonites are dirtier than ball clays but since the amount needed is so small it is not an issue. Bentonites are used in porcelain casting bodies to add leather hard strength and shrinkage to enable them to pull away from the mold.

Whiting or Calcium Carbonate: Normally small additions of this are employed (e.g. 5%). Many people think it is used to whiten the color, but not so. Whiting reduces a phenomenon called 'moisture expansion', causing glazes that are otherwise fitting to be stretched and therefore craze. The mechanism of this could be increasing the open porosity of the fired matrix, giving water a way to more quickly channel out when pieces are heated. It is also thought to assist in the development of crystal species that increase thermal expansion.

Safety

Talc is a magnesium silicate, either fibrous (like asbestos) or platy (like kaolin). Platy talcs are the ones that are useful in ceramics and producers make great efforts to insure the purity of their products (platy only). Ball clays contain significant quartz. Dolomites are not hazardous.

The Recipe

Use this recipe as a starting point. For the casting version start using the amount of water and deflocculant shown. Note that slip casting recipes that show water and deflocculant do so in terms of the total clay content. Thus 45% water means that for 100 pounds of clay you need 45 lbs of water. It is very valuable to understand the principles of deflocculation to properly tune this recipe to your materials and water supply.

A Typical cone 06-04 Ceramic Slip

Talc 50.0
Ball Clay 50.0
Water 45.0% of dry amt
Soda Ash 0.1% of dry amt
Sodium Silicate 0.2-0.4% of dry amt

If crazing is a problem: Use more talc and less ball clay (some people use a 60:40 talc:ball clay mix for casting). Be aware that commercial glazes do not all have the same thermal expansion, some will fit better than others. Test the transparent version of their glaze first.

Depending on the type of ware you make and glazes employed, you may have the option of firing higher (thus getting an improvement in strength). Lots of commercial glazes will handle up to cone 03.

Slips, engobes: At low temperatures these may not stick to the body very well unless you tune them to fit specifically and apply them at leather hard stage.

Commercial underglazes don’t develop a glassy phase at low fire so they do not bond well with the body. Consider testing different brands, they are not created equal. Or, better yet, make your own.

Related Information

Mural made using talc body and underglazes only


This picture has its own page with more detail, click here to see it.

Anti-racism themed, this was a project by students in a school in Vancouver, BC. The clay is Plainsman L213, a talc-ball clay body. Spectrum underglazes. Pieces were fired at cone 04.

Mosaic by Sikiu Perez


This picture has its own page with more detail, click here to see it.

Low temperature white talc body with bright glazes.

High thermal expansion talc body cannot be COE-calculated


This picture has its own page with more detail, click here to see it.

Talc is employed in low-fire bodies to raise their thermal expansion (to put the squeeze on glazes to prevent crazing). These dilatometer curves make it very clear just how effective that strategy is! The talc body was fired at cone 04 and the stoneware at cone 6. The former is porous and completely non-vitreous and the latter is semi-vitreous. This demonstrates something else interesting: The impracticality of calculating the thermal expansion of clay bodies based on their oxide chemistry. Talc sources MgO and low fire bodies containing it would calculate to a low thermal expansion. But the opposite happens. Why? Because these bodies are composed of mineral particles loosely sintered together. A few melt somewhat, some change their mineral form, many remain unchanged. The body's COE is the additive sum of the proportionate populations of all the particles. Good luck calculating that!

A low-fire talc body lacks plasticity when slip-mixed, but not when pugged


Talc body splitting in the plastic state

This picture has its own page with more detail, click here to see it.

This clay was slurried in a mixer and then poured onto a plaster table for dewatering. During throwing it is splitting when stretched and peeling when cutting the base. Yet when this same clay is water-mixed and pugged in a vacuum de-airing pugmill it performs well. One might think that the slurry mixer would wet all the particle surfaces better than a pugmill - that is our typical experience. However, it appears the energy that a pugmill can inject into the mix is needed to develop the plasticity when there is a high talc percentage in the recipe.

How to make a ceramic time-bomb


This picture has its own page with more detail, click here to see it.

This mug is pinging loudly and literally self-destructing in front of my eyes! Why? The glaze is under so much compression (the inside is pushing outward, the outside inward). Spiral cracks are developing all the way up the side. Small razor-sharp flakes are shivering off convex contours. Why? I accidentally fired a low-temperate talc body at cone 6 (the glaze is the Alberta Slip base cone 6 glossy). The clay body is not overly mature, but it just has an extremely high thermal expansion (talc is added to increase the expansion to fit low fire commercial glazes, they would craze without it). Shivering is serious, it is a mismatch of thermal expansion between body and glaze. It can happen at any temperature.

Are you firing a white talc body to cone 04 for durability. You are not getting it!


This picture has its own page with more detail, click here to see it.

Cone 04 is higher than cone 06 but ware is still very porous and weak. While it might be able to withstand handling, it may not be able to withstand being burst by its own glaze. Or shivering. Or crazing. Consider using a terra cotta with an white engobe. Fire to cone 03. This piece has a black engobe on the outside and a glaze under compression on the inside.

This talc artware body looked white...

Until I put it beside a cone 04 porcelain!


Porcelain clear glaze at cone 04

This picture has its own page with more detail, click here to see it.

On the right is L213, a body made using Texas talc and Kentucky ball clay. On the left is L3778H, a translucent cone 6 porcelain made using Grolleg kaolin, Nepheline syenite and silica. These test tiles were in the same cone 04 firing. Since both of these bodies have similar porosities and fired strengths at cone 04, does that mean one could use the porcelain? It appears the answer is yes. Why is that again? Because low-temperature artware clay doesn’t need vitrification; all the bodies are porous.

What could make this work? This crystal clear glaze, G1916QL1, fits the L213 but crazes after a few days on the porcelain. Increasing the firing temperature to cone 03 extends that time to 3 weeks. Cone 02 would likely extend it further. Adjustments to the glaze recipe (e.g. 400 mesh silica and increasing its percentage) would lower the thermal expansion and improve fit even more. This whole scenario is doable for DIY potters who mix their own bodies and glazes, especially for casting. The materials to make the porcelain are kaolin, silica and feldspar, even inexpensive kaolins would produce a body almost as white as this one at low fire.

The strange vitrification profile of a talc body


This picture has its own page with more detail, click here to see it.

This body is made from approximately 50:45:2:3 ball clay:talc:whiting:bentonite. These SHAB test bars are fired from cone 2 to 9 oxidation and 10 Reduction (bottom to top). From them the porosity and fired shrinkage can be measured (the SHAB test). Notice that the fired shrinkage is pretty stable from cone 2 to 8, but accelerates at cone 9 oxidation. But in reduction this stage has not been reached yet. The same thing happens with porosity, the cone 9 bar is dramatically more dense than the cone 8 one. But in reduction, it is still porous.

White Talc Artware Clay vs Terra Cotta:

The difference goes far beyond color


This picture has its own page with more detail, click here to see it.

These two sets of SHAB test bars are fired from coldest to hottest (bottom to top) through the range from cone 04 up to cone 4. The graph shows the decreasing porosities (water absorptions) and increasing shrinkages as temperature rises. Note the terra cotta reaches maximum shrinkage and minimum porosity at 2000°F (above which it begins expanding and melting). The talc body, by contrast, slowly matures, reaching a minimum porosity of 7% at 2150°F. It thus only sinters, never reaching a state of anywhere near the maturity and strength of the terra cotta. Clearly, the latter is not only high in iron oxide, but also in fluxes (like K2O, MgO, Na2O, CaO, etc) - these are responsible for how fast it vitrifies. The point where maximum fired strength is produced is the third bar up, 1970°F on the graph. However, there are multiple issues: Ware will warp in the kiln, the terra cotta red color has been lost and LOI gases of decomposition will disrupt glazes (with bubbles, blisters and pinholes). The most practical temperature is the second bar up, adequate density, good color, better quality glaze surfaces. The talc body? Although it fires to poor maturity across the range, it has one trump card: It provides a good base for glazes, producing bright colors and no bubbles.

Inbound Photo Links



Medium fire white bodies used at cone 04. Is that smart?


Stilts not always needed when firing artware pieces with glazed bottoms

Artware and stoneware pottery mugs
Which is better for hobby functional ware? Cone 04? Cone 10 reduction?

Links

Glossary Terra Cotta
A type of red firing pottery. Terra cotta clay is available almost everywhere, it is fired at low temperatures. But quality is deceptively difficult to achieve.
Glossary Low Temperature Glaze
In ceramics, glazes are loosely classified as low, medium and high temperature. Low temperature is in the cone 06-2 range (about 1800F-2000F).

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy