0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Rate | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | LAS Body | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Interaction | Oxide Molecular Formula | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Molecular Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Dipping Glaze

In traditional ceramics and pottery dipping glazes can be of two main types: For single layer and for application of other layers overtop. Understanding the difference is important.

Key phrases linking here: dipping glazes, dipping glaze, dip-glazed - Learn more

Details

Dipping (or pouring and draining) is the preferred method for single-layer application of glazes on bisque-fired pottery, it is fast and coverage can be very even. When the slurry has the right thixotropic behaviour drying time can be measured in seconds! Glazes for dipping usually contain little or no CMC gum, suspending and hardening happen solely because of clay(s) in the recipe. 15-25% raw kaolin, ball clay or Gerstley Borate are typical in glazes having good working properties (a small addition of bentonite can be used in recipes having inadequate clay). People using dipping glazes tend to weigh out and mix their own recipes. Dipping glazes are available commercially but they are often just brushing glazes with no Veegum (they still drip-drip and take a long time to dry). But they do require CMC gum to harden because of the high percentage of frit. Their working properties are so poor in comparison to a thixotropic slurry that inexperienced potters or hobbyists, for example, can be soured on the whole idea of dipping!

For multi-layering, that is, applying other layers over a dipping glaze (with no firings done between), a base-coat dipping glaze is needed, one that contains a binder to fix it well to the body and harden it on drying. Binders are much more effective if the glaze has plenty of super-fine particles for them to bind with (thus bentonite additions are common in glazes containing CMC gum). These glazes dry slower, go on thinner, and drip a lot during draining.

On this website, most of the articles and reference material assumes the making of single-layer dipping glazes (unless otherwise mentioned). We promote understanding the relationships between recipes (of materials) and their oxide chemistry with what happens in the kiln. And the concept of recipe limits. Weekend warrior type potters are typically more interested in buying commercial bottled and gummed products and exploring all the colors and interactions of multilayering with them. Industry also has minimal interest in this type of glaze, not only because their formulations contain lots of frit, but because their machines and process also demand the use organic and inorganic additives.

Pre-Mixed Powdered Dipping Glazes

These products are manufactured by various companies and can be challenging to support. For instance, one brand recommends adding some of the water, letting it sit for 20 minutes, and then mixing for 30 seconds. After that, sieve, let it sit overnight, mix again, and handle the possibility of hard panning (adding their Suspendaid product if needed). Mix again, repeat cycles of checking specific gravity (targeting 1.39-1.41) and adding small amounts of water until the target specific gravity is reached, perform 5-second dipping tests to verify the thickness, and finally fire the tests. Users who undertake all of this might decide to add another step by weighing out the powders using their own recipes. Specific gravity targets range from below 1.4 to above 1.5, and there’s no mention of achieving a thixotropic slurry. The emphasis seems to be on achieving a consistent dipping time. They also warn against layering (for the same reasons mentioned here). Notably, I’m not aware of anyone who provides instructions for mixing as a first-coat dipping glaze. If you try mixing one of these as a thixotropic slurry, please let us know how it worked and at what specific gravity. If you had to add a cup of SuspendAid to prevent hard panning, how did that not push the specific gravity too low, and did it work?

Related Information

Commercial brushing glaze on a non-gummed dipping glaze: Crawling


This picture has its own page with more detail, click here to see it.

Non-gummed dipping glazes go on evenly and dry quickly on bisque ware (if properly gelled). But they only work well as a single layer. If you try to paint commercial gummed brushing glazes over them the latter will compromise their bond with the body, cracks will develop during drying and bare patches like this will result during firing. For multi-layering the base dipping glaze must be gummed (e.g. 1% CMC gum). It will go on thinner, drip longer and dry much slower, but that is the price to pay if you want to layer over it.

CMC Gum is magic for multi-layering, even for raw Alberta Slip


A glaze that cracks on drying was fixed

This picture has its own page with more detail, click here to see it.

The glaze on the left is 85% of a calcine:raw Alberta Slip mix (40:60). It was on too thick so it cracked on drying (even if not too thick, if others are layered over it everything will flake off). The center piece has the same recipe but uses 85% pure raw Alberta Slip, yet it sports no cracks. It should be cracked much worse than #1. How is this possible? 1% added CMC Gum (via a gum solution) was added! This is magic, but there is more. It is double-layered! Plus very thick strokes of a commercial brushing glaze have been applied over that. Yet no cracks. CMC is the secret of dipping-glazes for multi-layering. The downside: More patience during dipping, they drip a lot and take much longer to dry.

Better to mix your own cover glazes for production?


This picture has its own page with more detail, click here to see it.

Yes. In this case, the entire outside and inside of the mug need an evenly applied coat of glaze. For hobby, this makes sense. But in production, cover brushing makes less sense. The right pail has 2 gallons of G2934Y base (the most expensive one I use) with 10% Cerdec yellow stain: $135 (in 2023). Cost of brushing jars with the same amount: $600+! And each jar logs 10-15 minutes of painting time plus waiting between coats. The one in the pail is a true dipping glaze, it dries immediately after dipping in a perfectly even layer (if mixed as a thixotropic slurry).

Can you brush a dipping glaze on to leather hard ware? No.


This picture has its own page with more detail, click here to see it.

The body needs to shrink as it dries. Typical glazes have low clay content and shrink very little. So as the body shrinks underneath the glaze just flakes off. Brushing glazes contain significant amounts of gum, that gum bonds them securely to bisque ware, but not to unfired ware. As you can see here. the glaze bond with the body could not withstand the differential during drying.

Commercial glazes on decorative surfaces

Your own on food surfaces


This picture has its own page with more detail, click here to see it.

These cone 6 porcelain mugs are hybrid. Three coats of a commercial glaze painted on the outside (Amaco PC-30) and my own liner glaze, G2926B, poured in and out on the inside. When commercial glazes (made by one company) fit a stoneware or porcelain (made by another company) it is by accident, neither company designed for the other! For inside food surfaces make or mix a liner glaze already proven to fit your clay body, one that sanity-checks well (as a dipping glaze or a brushing glaze). In your own recipes you can use quality materials that you know deliver no toxic compounds to the glass and that are proportioned to deliver a balanced chemistry. Read and watch our liner glazing step-by-step and liner glazing video for details on how to make glazes meet at the rim like this.

Think the idea of mixing your own glazes is dead? Nope!


This picture has its own page with more detail, click here to see it.

These are two pallets (of three) that went on a semi-trailer load to a Plainsman Clays store in Edmonton this week. They are packed with hundreds of bags of powders used to mix glazes. More and more orders for raw ceramic materials are coming in all the time. Maybe you are using lots of bottled glazes but for a cover or a liner glaze it is better to mix your own. And cheaper! And there are lots of recipes and premixed powders here to do it. One of the big advantages is that when you dip ware into a properly mixed slurry it goes on perfectly even, does not run and dries on the bisque in seconds. No bottled glaze can do that.

I have 161 grams of stain. I need to mix it into how much clear glaze slurry?


This picture has its own page with more detail, click here to see it.

Stain powders are expensive. I want to make as much glaze as I can from every gram of this red stain I have at hand. I have weighed a teaspoon of my clear glaze liquid slurry (recipe G2926B). I dried it out under a heat lamp and weighed it again (top left). I have filled those two weights, 8.9 and 4.74, into a spreadsheet I made. It calculates the proportions of water and powder in the glaze slurry. I have filled in "10" for the percent of stain needed. It is telling me I need to mix the stain into 3040 grams of the liquid glaze. That gives me about 5 pints of glorious bright-red dipping glaze. The dipping process enables me to apply it so much more evenly than I can do by paint-on methods (provided that I have the right specific gravity and thixotropy). And, I got this much glaze for about $50 worth of dry materials (vs. $20 for a pint of paint-on glaze).

Inbound Photo Links


Three containers of glaze slurry
Prepare your own glazes for three application methods

Transparent glazed mug and jar
The glaze cost on this mug is three times the cost of the clay!

Links

Glossary Brushing Glaze
Hobbyists and increasing numbers of potters use commercial paint-on glazes. It's convenient, there are lots of visual effects. There are also issues compared to dipping glazes. You can also make your own.
Glossary Base-Coat Dipping Glaze
These are ceramic glazes intended for dipping but which contain a gum to enable them to adhere to the body better and tolerate over-layers without danger of flaking or cracking.
Glossary Limit Recipe
"Recipe logic" is the ability to sanity-check ceramic glaze recipes on sight, by noting that materials present and their relative percentages.
Glossary Thixotropy
Thixotropy is a property of ceramic slurries of high water content. Thixotropic suspensions flow when moving but gel after sitting (for a few moments more depending on application). This phenomenon is helpful in getting even, drip-free glaze coverage.
Glossary Spray Glazing
In ceramic industry glazes are often sprayed, especially in sanitary ware. The technique is important.
Glossary Dip Glazing
A method of applying glaze quickly and evenly to pottery.
Glossary Glaze Layering
In hobby ceramics and pottery it is common to layer glazes for visual effects. Using brush-on glazes it is easy. But how to do it with dipping glazes? Or apply brush-ons on to dipped base coats?
URLs https://insight-live.com/uploads/potters_choice_dry_dipping_instructions.pdf
Potters Choice dry dipping glazes, add water and go
These are sold as pails with 10lb powder. These detailed instructions and videos explain how to add the water, get the right specific gravity (1.38-1.5), mix, maintain and use the products. Slurry and application properties span a much wider range than their Celadon line.
URLs https://amaco.com/asset/67c856372d9e6
AMACO Celadon powdered dipping glazes - Mixing instructions
Sold in pails with 10 lbs of powder. They recommend 1.41-1.43 specific gravity, distilled water, intense mixing, five second dip, no layering, dime thickness.
URLs https://www.instagram.com/reel/Db6gU0fCuMZ
Factory worker glazing bone-dry plates by spinning, sponging and dipping
The plates appear to be heated and the glaze is likely high-specific gravity because it dries incredibly fast.
URLs https://www.facebook.com/share/r/1FFFTP31rW
Factory worker using wire dipping tongs to apply very thin glaze on bisque ware.
The factory slurry is very watery and requires continuous stirring.
URLs https://www.facebook.com/share/r/1Z3hf7YFU4
Dipping glazing: An art in factories
Rims, outsides only, plates, fountains and clever techniques using very watery glaze on bisque.
URLs https://www.facebook.com/share/r/1DjFuEd4Bj
A factory worker dip-glazes a large platter.
A clever tong tool that does not disturb any surfaces.
URLs https://www.facebook.com/reel/1084612477351344
Factory worker dip-glazes mugs
A skilled worker uses a custom dipping tong to thick-layer the outsides and thin-layer the insides. Notice how thixotropic the glaze is.
URLs https://www.facebook.com/reel/1555758769633769
A factory worker dip-glazes translucent porcelain plates with her bare hands. Very fast!
She works at incredible speed, glazing one every two seconds. Without using dipping tongs. She applies a very thin layer of transparent glaze. While it appears very watery (low viscosity), it is likely high-solids and deflocculated to achieve extreme thixotropic behavior (fluid when moving, gelled when still). The speed of the dip, and fluid sweep while below the surface, ensure that all parts of the plate spend the same fraction of a second submerged, ensuring a uniform layer. Notice also that the plates on the split foam belt dry enough to stack within 10-15 seconds. What about the spot on the rim where she is holding it? Upon pulling the plate out, the glaze is still fluid enough to pool over it as a product of the way she releases it. Notice also that she picks them up with a glove, which means they may be hot (to speed drying). Finally, additions of surfactants and defoamers break the surface tension, enabling air bubbles to pop and smooth over quickly before the glaze dries. One final detail deserves repeating: This is translucent porcelain, maybe even bone china. That means the ware has been bisqued to zero porosity. Wow!
URLs https://www.facebook.com/reel/2146510669231542
Factory worker dip-glazes large bisque casseroles in thixotropic glaze
Notice the special dipping tong. And the glaze has been tuned to have the rheology needed to not over-thicken. This enables the worker to grab the already-dried first extracted portion of the rim to stabilize the piece as it is pulled completely out of the slurry.
URLs https://www.instagram.com/reel/Ddd9ih8Fd2w
Factory worker dip-glazes a plate with bare hands
The rim holding spot has been preglazed.
URLs https://www.facebook.com/reel/1369572738697142
Factory worker dip-glazes the outside of a teapot
URLs https://www.facebook.com/share/r/1FfzUaLsev
Factory worker dip-glazing using a special tool
It is a small bowl with an intricate wax resistant design. The dipping tongue doubles as the holder for drying.
URLs https://www.instagram.com/reel/DdYHCPgyt6z
Factory worker and machine dip-glazing mugs

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy