0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Rate | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition During Ceramic Firing | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | DTA Test | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | LAS Body | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | LOI-Adjust | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Interaction | Oxide Molecular Formula | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | TGA Test | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Molecular Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Liner Glazing

Step-by-step to apply inside and outside glazes to a pottery mug and get them to meet at a clean line at the rim.

Key phrases linking here: liner glazing step-by-step, liner glazing, liner glazed - Learn more

Details

Mug has been liner glazed, waxed and cut/trimmed but not yet sponge-cleaned for dipping the outer glaze

This page describes the technique of glazing pottery to make an inside and outside glaze meet in a clean line at the rim. The technique is common in commercial ware and requires precision to execute well. It is not only aesthetic but also functional - more durable and food safe glazes are appropriate on food surfaces. Separate glazing operations for inside and outside surfaces are also a practical production technique (e.g. for thin-walled pieces that would waterlog on a complete dip, where separate people or teams cooperate in glazing each piece).

Step-by-Step

  1. Fill the bisque mug with liner glaze. Pour it out in a circular motion and then dip the lip. Hold it there long enough to get the thickness needed:
  2. After the glaze has dried sufficiently, use a banding wheel to wax up the inside (starting about an inch down) and just up around the top of the lip.
  3. Using a sharp knife (e.g. Olfa cutter) in one hand and rotating the mug with the other, cut away the glaze (down to the bisque) up to the highest point on the lip (the best cut with the least dust is done when the glaze is still damp). Clean up any remaining glaze around the outside of the rim using a fettling knife. Now the inside glaze terminates at a perfect wax-covered edge at the lip.
  4. Using a damp sponge, clean any remaining glaze off the outside up to the wax line. This is not always necessary, but note that the poorest surface to receive the outer glaze is one that is dry and has residue from not being cleaned off completely (pinholes and crawls occur). The second poorest surface is one that has residue but is still too wet from the inside pour (often true if the piece is thin walled). The best surface is one that is slightly damp and clean.
  5. Glaze the outside. Keep your hands damp so they will not stick to the wax (and pull off sections as you touch it). Push the lip of the mug into the glaze 5-10mm (being careful to hold the mug level as you do this). Shake off the drips and immediately turn it over, put your hand inside, clamp against the inner surface and push it into the glaze right down to the rim (to overlap the lip dip just made). It may be tricky at first to push the mug down far enough and avoid glaze spilling inside.
  6. Set the mug on a turntable to sponge away any drips left over the wax-covered areas on the inside top of the lip.
  7. Clean the foot and set it out to dry.

Related Information

Liner Glazing a porcelain mug

The process of applying a liner glaze to the inside of a piece (by pouring), applying wax emulsion up the top inside and over the rim (using a turntable and brush), removing the glaze up the outside to mid-rim and finally dipping the rim and outside into the other glaze.

Meet two glazes at the rim using wax emulsion. Why? How?


Liner glazed mug

This picture has its own page with more detail, click here to see it.

Reactive glazes (melt-mobile, crystallizing or heavily pigmented) are the least suitable for food surfaces because they have the potential to leach metals. Liner glazing ware is an excellent way to deal with this problem. Not only does this approach improve functionality but it can be aesthetically pleasing and practical in production.

This liner is GA6-B, a pottery glaze recipe we promote with confidence. Not only is it less likely to be leaching metals but also less likely to craze - this assures water tightness on non-vitreous bodies and eliminates any potential for bacteria growth in the cracks (especially if the body has porosity). Unfortunately, glazes that leach are also likely to stain and cutlery mark - these add more reasons why they are most often unsuitable for food surfaces.

The straightness of the dividing line is affected by both the application technique and the degree to which the two glazes bleed into each other and run. Read and watch our liner glazing step-by-step and liner glazing video for details on how to do this - it is practical for any potter or hobbyist (or even in production). And tap/click the picture above for other examples of this.

Beautifully finished mug from Tim Hortons


Tim Hortons coffee mug

This picture has its own page with more detail, click here to see it.

This was a limited edition heavy (450g or 1 lb) white stoneware mug for sale in Tim Hortons restaurants recently. It exhibits fine workmanship and carries lessons for potters. Notice they employ a transparent food safe liner glaze. The outside decoration appears to have been done at the leather hard stage using a colored engobe, wax resist and ceramic transfers. The entire piece was likely dipped in a transparent glaze (in the bisque state). The handle has a simple and functional shape that could be emulated using our handle mold making techniques. The simple flared body shape lends itself well to jiggering.

Mistake when liner glazing a mug


This picture has its own page with more detail, click here to see it.

The white inner liner glaze (that wraps over the rim) was not removed after the wax was applied. The outer glaze thus overlays patches of it near the rim. The meeting line has been blurred and the other glaze has run downward and crawled somewhat revealing patches of the inner one.

Liner glazing done right and wrong


This picture has its own page with more detail, click here to see it.

I already know that many with say they prefer the one on the right. However, the purpose of my liner glazing is to minimize liquid contact with glazes strongly pigmented with heavy metals. With the proper technique of applying a liner glaze, you can make the outside and inside ones meet in a straight line at the outer part of the rim rather than just have one spill over the other.

A fluid melt glaze bleeds much more into adjoining ones


This picture has its own page with more detail, click here to see it.

The outer green glaze on these cone 6 porcelain mugs has a high melt fluidity. The liner on the upper mug is G3806C, a fluid melt high gloss clear. The liner glaze on the lower one, G2926B, is high gloss but not highly melt fluid. Thus, when both the outer and inner glazes have high melt fluidity (upper mug), they bleed together forming a fuzzy boundary. But when even one of them is not, a crisp boundary is achieved (lower mug).

Inbound Photo Links


Mother Nature's porcelain black mug
Gunmetal black mug demos liner glazing: Safe glaze inside, pigmented matte outside.

Links

Glossary Liner Glaze
Liner-glazing is a way to assure that your ware has a durable and leach resistant surface. It also signals to customers that you care about this.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved