0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Interaction | Oxide Molecular Formula | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Molecular Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Ceramic Decals

This process of printing a design (using ceramic inks) onto film-coated paper to create a waterslide transfer. On wetting, the film decal can slide off the backing on to the glazed ware.

Key phrases linking here: ceramic decals, decal - Learn more

Details

A method of printing designs (using ceramic inks) onto a transparent film, then transferring that to glazed ware (most commonly known as waterslide transfers). The film has a glue that holds it to a heavy opaque paper backing coated with a glossy release layer. On wetting (for the correct amount of time), the glue loosens and enables the transfer. As the decal dries on the ware the glue holds it in place. When fired, the very thin film backing material burns away leaving the ink to bond with the glaze surface. The film can accommodate quite a bit of irregularity in the contours of the surface.

Making these inks and silk screening the decals is typically beyond the ability of small manufacturers or potters. The inks are formulated to fuse as low as possible, which can be as low as cone 015 (the know-how to formulate compounds that melt that low is not common). Nowadays decals can be printed directly in an inkjet printer (fitted with ceramic ink cartridges), a laser printer (fitted with ceramic toner), or by silk screening (the latter transitioning to the former in recent years). These new technologies have many obvious advantages, and, some disadvantages. It goes without saying that complicated printer hardware, especially if it has been adapted to inks or toners made using abrasive ceramic powders, will have issues. The troublesome nature of running this equipment and the expensive supplies are the reasons why decals from online service providers are so expensive.

Where can you have decals printed? Etsy.com is likely the best place. A search phrase like "custom ceramic waterslide decals" should find them.

Some manufacturers of traditional ink formulations, mediums, silk screening, and ceramic waterslide decals have gone out of business in recent years and this has caused problems for companies who depend on them. Their formulations were lost in the process, notwithstanding that, the silkscreen decal process is still very useful. Are you an engineer who knows about these formulations? Would you be willing to share these with us so we can help others? Please contact us.

The inks and toner powders are specialized formulations of nano-powdered frit (bismuth-based) and stains, they form a glassy color at very low temperatures. However, since the designs are on the glaze surface, they must endure the full forces of wear and tear to which the piece is exposed. Since these inks do not contain the stable silicates that a glaze does (because they need to melt so low), they are more subject to abrasion and degradation. Decal firings only go to around 1600F (each decal manufacturer will have specific instructions). The underlying glaze usually does not melt enough to bleed their edges. This stable surface enables great precision of design, full-color photos can thus be produced. That being said, the colors are not as accurate as regular print, only a subset of the CMYK color set can be printed (and even a smaller subset of the RGB colorset used on video monitors).

Firing decals on large pieces can put you on a collision course with ware cracking - resulting from stresses in passing up or down too fast through quartz or cristobalite inversions. It is a necessity to have a programable kiln controller to slow down through these periods.

There is a serious issue to think about if you are planning to introduce decals into your production, decal-printing websites seldom even mention this. Many glazes are reactive fluid melters (high boron, zinc, lithium) and begin to soften at decal temperatures. These will often form pits, pinholes or even blisters during the firing-on of the decal, ruining the piece. The higher you fire the ware originally and the later the glaze melts, the less likely this problem will be. Even if it does not melt, the glaze may have a visual character (color or surface texture) that is a product of crystallization during cooling, these crystals could easily be affected during a decal firing. Thus, low-fire glazes will, of course, be most susceptible to this. Mid-temperature glazes having the lowest possible B2O3 content, yet still melting enough, will be more likely to work. Cone 10 ware will be even better/ fast fire glazes melt late and will thus work the best.

Related Information

Gold decal on a gunmetal matte black glaze


Black mug with gold flower

This picture has its own page with more detail, click here to see it.

This is a cone 6 porcelain mug with G2934 matte glaze (with 6% black stain added). We get this satin matte effect in our test kilns using the PLC6DS schedule. Larger kilns cool slower so this glaze turns out too matte in them, we deal with that by increasing the percentage of glossy base (this is a 15:85 blend of G2926B glossy and G2934 matte). The gold decal is from Sanbao Studio. On the left, it has just been applied, other than the glossy finish revealing its location, no gold design is visible. But, after the decal firing, using the MDDCL schedule, we get the result on the right.

The G2934 base matte recipe is good for decals because it has a very low B2O3 content (unlike high boron glazes that can begin to melt very early, even in a decal firing, and alter their degree of matteness or even produce tiny pinholes or blisters). G2934 can tolerate some high-boron G2926B glossy, enough to de-matte it, and still work well with decals.

Decal on a raw body surface


This picture has its own page with more detail, click here to see it.

Fired in a standard decal firing. The glaze on the tile has helped fuse it to a glossy surface. Has worked well except for adhesion problems during application (because the porous body adsorbed all the water immediately). If the tile had been soaked previously it would have been better.

What is that glossy square around the decal?


This picture has its own page with more detail, click here to see it.

An example of a digital decal that has been fired at 1500F onto a magnesia matte cone 6 glaze. Notice the glossy, square around the graphic. This is where the decal paper was cut prior to transfer. The glossy layer is by design, this decal paper has a thin layer of glaze and the inkjet design is printed, reverse reading, onto that. After transfer and firing the thin glaze layer insulates the color from coming into contact with anything that might leach it. We normally cut around designs so that the glossy pattern does not detract from the appearance (as it does here). Typical decals don’t have the glaze covering, the pigments melt and fuse directly with the underlying glaze surface. These are important to preserve matte surfaces.

Why did this piece come out of a decal firing crazed?


Crazing mug after decal fire

This picture has its own page with more detail, click here to see it.

This Cone 10 matte mug has been refired to attach decals. The fired matrix of the body is now brittle and dense and contains millions of quartz grains of many sizes. During the refire up through quartz and cristobalite inversions each of them experiences sudden volume increases. This does not happen in the glaze because its quartz particles were dissolved in the melt and converted to silicates during the previous glaze firing. The suddenness of the expansion depends on the rate of temperature increase and its extent depends on the size of the quartz particles. The body's passage through these two zones stretched the glaze and cracked it. Had the glaze fit been better (under some compression) it would likely have been able to survive.

Why has this platter has cracked in half during a decal firing?


This picture has its own page with more detail, click here to see it.

Your ware is fairly thick. It was already vitrified in a previous firing. It now must climb and fall through quartz and cristobalite inversions during a decal firing. The firing schedule provided by the decal supplier ramps up very quickly. The result? A cracked piece.

Can a decal firing melt a glaze? Yes!


Decal firing pits the glaze

This picture has its own page with more detail, click here to see it.

Typical zero-boron high-temperature glazes will not soften in a 1500F decal firing. But low-temperature glazes will (especially those high in boron). Even middle-temperature ones, especially those having significant B2O3, can soften. G3806C (right), for example, is reactive and fluid, it certainly will. Even G2926B, which has high Al2O3 and SiO2, has tiny pits (because of the amount of B2O3 in contains). In serious cases, they can bubble like the mug on the right. What happened to this one? Steam. It was in use and had been absorbing water in the months since it was first glaze-fired at cone 03. The one on the left was not used, but it did have some time to absorb water from the air, it is showing tiny pits in the surface. Even if moisture is not present, on refire low fire bodies continue to generate gases of decomposition that affect glazes. Each decal manufacturer has a recommended firing temperature, that is for their decals, not your glaze.

Inbound Photo Links


Ceramic stones
Making ceramic "stones that cry out"

Links

Glossary Silk screen printing
Silk screen printing is one of the best options for hobbyists and potters to reproduce crisp and detailed decoration. But there are many details to know.
Glossary Ceramic Ink
You can make your own ink (or buy it) and apply it to ware using various methods (e.g. rubber stamping, silk screen, inkjet decals).
Glossary Ink Jet Printing
Ink jet printed decoration is now pervasive in all parts of the ceramic industry. And in hobby also.
Glossary Cristobalite Inversion
In ceramics, cristobalite is a form (polymorph) of silica. During firing quartz particles in porcelain can convert to cristobalite. This has implications on the thermal expansion of the fired matrix.
Glossary Quartz Inversion
In ceramics, this refers to the sudden volume change in crystalline quartz particles experience as they pass up and down a temperature window centering on 573C.
Glossary Ceramic Transfer
URLs https://ceramicartsnetwork.org/shop/ceramic-transfer-printing/
Ceramic Transfer Printing 144 page book available at CeramicArtsNetwork
Book on how to formulate colors and print on to water slide transfer paper.
URLs https://ezscreenprint.com
EZScreen Silk Screen kits
Their method enables printing on to stencils (using an inkjet printer) and sunlight-exposing the clear film on to pre-emulsified stencils.
URLs https://cerprint.com/
Ceramic laser printers and toner cartridges
As of 2021 these printers are now available for less than $1000. Cartridges are $500 for each color.
URLs https://www.digitalceramics.com/in-glaze-high-temperature-transfers
Inglaze High Temperature Transfers
The pigments can be fired at very high temperatures of 1100ºc - 1300ºc to ensure they sink into the glaze, improving durability and resistance. Ideal for the more demanding hotelware market.
URLs https://www.instagram.com/reel/DaB9ut2SrA7
Skilled factory worker applies full side decal to coffee cups
URLs https://www.instagram.com/reel/DdOnoqZR633
Factory worker rapidly applying decals
URLs https://www.instagram.com/reel/DdSzyTBvFRO
Factory worker quickly applying full decal to outside of mug
URLs https://www.instagram.com/reel/DeHSu3zxZuh
Factory worker demonstrates how forgiving a decal can be when being placed

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy