0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Rate | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition During Ceramic Firing | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | DTA Test | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | LAS Body | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | LOI-Adjust | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Interaction | Oxide Molecular Formula | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | TGA Test | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Molecular Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Spray Glazing

In ceramic industry glazes are often sprayed, especially in sanitary ware. The technique is important.

Key phrases linking here: spraying glazes, spray glazing - Learn more

Details

In the production of smaller bisque fired ceramics it is almost always possible to dip-glaze ware. However, this is seldom an option for single-fire ware (especially if large). This is the case in the sanitary ware industry, for example. Spraying is the only option, and it is a very effective one if done properly. Typically, opacified glossy glazes of high specific gravity (up to 1.8) are employed, the low water content speeds drying (thixotropy is not generally a concern, low water content is the main issue). Potters are much more flexible and less demanding when spraying. They typically spray a water-thinned slurry on porous bisque ware that is very forgiving of runs and drips.

For best results in pottery and hobby:

-Glazes need enough clay to suspend and harden them, but not so much that they dry too slowly or shrink too much (thereby cracking or flaking off). 10-20% should be OK.
-Gravity-feed guns are the most trouble-free.
-Use a sticky kaolin as the clay portion (e.g. Grolleg, NZK).
-For lower specific gravity glazes, adjust the slurry so that it is thixotropic, that is, so it stays in suspension in the sprayer.
-Use glazes high in frit and low in troublesome raw materials (ones that affect slurry viscosity or thixotropy, are soluble and crystallize in the slurry, create a precipitate scum inside containers or ones that contain excessive particulates).
-Use the right frits. They need to source the needed fluxing oxides and complement the recipe to optimize clay percentages. For example, if a glaze needs more clay then the frits employed should have lower Al2O3 content so that can be sourced from a kaolin instead (or vice versa).
-Ball mill your glazes or sieve them enough to be sure there is no particulate matter.
-Spray ware when it is sill warm or even hot to encourage fast drying.
-Make sure ware is thick enough so it can absorb plenty of water.
-Make sure your spray operator is skilled and has good equipment. Spray an even layer. Start at the bottom and work upward. Be careful about over-spraying already-dry areas, if done excessively this can rewet them and cause lifting during drying (and crawling during firing).
-Spray the ware on a rotating turn-table having a knobby or spiked rubber or plastic mat on which to set the item.
-Use a good quality stainless steel agitated pressure pot sprayer.
-Apply the thinnest possible layer needed to get the desired fired effect.
-Incorporate CMC gum, if needed, to improve bonding to bisque, dry hardening and smooth out.

Again, the rheology of your slurry is important for quality, efficiency and avoidance of production issues. Experiment as needed. Document the slurry preparation, measurement and maintenance procedures well.

For good spraying technique watch the video provided below. It was graciously given to us from http://shower-shelf.com. They also document their vibratory glaze sieve on youtube (links below for it and where to get the vibration motor).

Related Information

Spray glazing a nitch shelf at shower-shelf.com

Notice he starts from the bottom and works his way upward.

Spray glazed large bowl with two glazes meeting-at-the-rim


This picture has its own page with more detail, click here to see it.

The inside glaze is G2571A, outside is the bamboo version of the same recipe (with added Zircopax and rutile). Clay: Plainsman H443. Firing: Cone 10R. No wax was needed for application yet the two colors meet at the rim in a straight line (the outside was sprayed last). We used a gravity-feed sprayer, 100ml of glaze was applied on both the inside and outside.

Links

URLs http://www.finishsystems.com/catpressurepots.html
CA Tech Paint Pressure Pots for Spray Glazing
URLs https://www.youtube.com/watch?v=0zXfghDNxUg
ShowerShelf.com vibratory screen that fits the top of a five-gallon bucket
The tank, sieve and vibration assembly are all in one piece that fits into the top of the bucket. This unit can handle 1.8SG slurry.
URLs https://www.amazon.com/Vibration-3600RPM-Industrial-Asynchronous-Vibrator/dp/B07P5CLJLP/ref=sr_1_12?qid=1559306388
Industrial vibration motor at Amazon.com
URLs https://www.luepottery.hwy.com.au/PDF/glaze%20spray.pdf
Glaze Spraying booklet by Roger Graham - Excellent reference
URLs https://www.smac.it/en/dettaglio.php?idprod=239
K-Flow automatic glaze flow rate controller for spray nozzles
The system will display the instantaneous flow of each individual nozzle and signal any anomalies by alarm or stop the production line or the application device to avoid glaze and material waste.
URLs https://www.smac.it/en/dettaglio.php?idprod=232
Versatile/Plus airless tile spraying machine
Available from 4 to 8 spray-guns with feeding by high-pressure pump for application of engobes, glazes and crystallines.
URLs https://www.smac.it/en/dettaglio.php?idprod=45
Airless pumps for glaze and engobe suspensions
Automatic, correct application of all the suspended products having high abrasion such as glazes, engobes and crystalline, maintaining a precise and constant pressure without pulsations.
URLs https://www.smac.it/en/dettaglio.php?idprod=29
Multicolor four color spray gun
System to spray chromatic effects in 4 different colors with one single spray-gun.
Glossary Specific gravity
In ceramics, the specific gravity of slurries tells us their water-to-solids ratio. That ratio is a key indicator of performance and enabler of consistency.
Glossary Viscosity
In ceramic slurries (especially casting slips, but also glazes) the degree of fluidity of the suspension is important to its performance.
Glossary Deflocculation
Deflocculation is the magic behind the ceramic casting process, it enables slurries having impossibly low water contents and ware having amazingly low drying shrinkage
Glossary Once-Fire
The practice of once-firing ceramics (no bisque) to produce fully glazed products. Considerable technical expertise and good testing are required to make it work. This is not a shortcut to skipping bisque firing.
Glossary Dipping Glaze
In traditional ceramics and pottery dipping glazes can be of two main types: For single layer and for application of other layers overtop. Understanding the difference is important.
Glossary Base-Coat Dipping Glaze
These are ceramic glazes intended for dipping but which contain a gum to enable them to adhere to the body better and tolerate over-layers without danger of flaking or cracking.
Glossary Brushing Glaze
Hobbyists and increasing numbers of potters use commercial paint-on glazes. It's convenient, there are lots of visual effects. There are also issues compared to dipping glazes. You can also make your own.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy