A powder carrier is the liquid vehicle that enables a ceramic powder mixture to be brushed, sprayed, poured, printed or otherwise applied.
Key phrases linking here: powder carrier - Learn more
A powder carrier is the liquid vehicle that enables a ceramic powder mixture to be brushed, sprayed, poured, printed or otherwise applied. The term is especially useful for underglazes, engobes, brushing glazes, ceramic inks and screen-printing pastes.
It should be distinguished from the ceramic medium. A ceramic medium is the inorganic formulation that hosts the stain or colorant and remains after firing. It can contain frit, feldspar, clay, silica, zircon or other ceramic materials to control melting, adhesion, opacity, thermal expansion and surface character. The powder carrier controls application and drying.
A typical colored product can thus be considered as having three parts:
In ceramic ink terminology, the powder carrier is often called the vehicle. The carrier must temporarily transform a powder into a usable liquid, paste or ink. Depending on the application method, it may need to:
No single carrier additive necessarily performs all these functions. For studio underglazes and brushing glazes, the liquid part is normally just water (vs oils, glycols, resins or organic solvents used in industry). The carrier can contain:
The simplest carrier may just be water (e.g. a dipping glaze). Others are carefully balanced systems of binder, gellant, dispersant, surfactant and preservative.
A practical development sequence to tune a DIY carrier is:
Unless blender mixing, CMC is normally easier to incorporate as a prepared solution than as dry powder (avoiding persistent lumps).
DIY glazes and underglazes permit the ceramic medium and the powder carrier to be optimized independently. The ceramic medium can contain only enough stain and melter to produce the required color, opacity and fired adhesion. The carrier can then be tuned for the actual application method instead of accepting the compromises necessary in a commercial product.
| Glossary |
Stain Medium
A stain medium (or ceramic medium) is a mix of powdered ceramic materials that impart ceramic properties that stain powders lack in themselves (e.g. ability to form a hard ceramic that fits the underlying body or overlying glaze. |