0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Rate | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition During Ceramic Firing | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | DTA Test | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | LAS Body | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | LOI-Adjust | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Interaction | Oxide Molecular Formula | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | TGA Test | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Molecular Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Zero4

The designation for a group recipes for body, glaze and engobe (by Tony Hansen), that potters can use to make low fire stoneware and fritware porcelain

Key phrases linking here: zero4 fritware, zero4 - Learn more

Details

Zero4 porcelain (code number L3924J ) is a fritware concept body designed during 2022 (it employs Ferro Frit 3110 as the flux instead of the feldspar used in typical porcelains; to get the recipe and more technical information and pictures, click that code number in the last sentence or Google "L3924J recipe"). Zero4 reaches zero porosity at cone 04 and looks, feels and performs like a fine porcelain. Because it vitrifies so early, bisque temperature is best around 1450F.

June 2024: Costs have skyrocketed since 2022; this prices out to $25/lb now for me! However, this body might still be feasible for making jewelry from colored porcelains.

The recipe is public so you can mix it for yourself. Zero4 is for potters who like to experiment with mixing their own clays; it involves weighing out the ingredients, mixing it as a slurry using a high-speed propeller mixer and then dewatering it on a plaster batt (actually, blender mixing is better; that will break down agglomerates). No clay body manufacturer that we know of sells anything that is even close to this (because it would be so difficult and expensive), so if you take the trouble to make it, you are creating very unique ware.

This is a follow-up to the Zero3 recipe; it is more vitreous and is targeted at working with standard low-temperature commercial glazes and underglazes. Zero4 porcelain has a companion glossy glaze recipe based on G1916Q. We are still assessing its long-term resistance to leaching.

Want the recipe and to learn more? Zero4 is code numbered L3924J; all the details along with information on the G1916Q3 base glaze are available. Could it go lower? Yes - with more frit or a lower-melting one. Could it go 200-300F lower? Yes, there are bismuth frits that can do that (but at an obvious cost).

Related Information

Zero4 fritware mugs fired at cone 04


Two porcelain hashtag mugs

This picture has its own page with more detail, click here to see it.

To a potter, it may seem impossible that a body can be this porcelain-like at such a low temperature. And that such a body can be as plastic as this is. Achieving these came at the cost of shrinkage, both drying and firing, 18% total (vs 14% of a Grolleg cone 10 porcelain). Using this Zero4 fritware, very thin-walled pieces can be thrown. The frit also produces a body having a higher thermal expansion, so it fits any low-temperature glaze we have tried. This glaze is G1916QL3 ultra gloss clear glaze on Amaco Velvet underglazes. The low temperature has another benefit: Very sharp edges on painted underglaze designs. Zero4 replaces my old Zero3 fritware with a body that works at a more common temperature. It also employs a tiny amount of blue stain to produce the bluish-white color. Like Zero3, you can also make this yourself.

Zero4 porcelain cup cross-section


This picture has its own page with more detail, click here to see it.

The fritware body is highly plastic and can be thrown very thin. At cone 04, this thin-walled mug did not warp even though it fired to a near-glasslike cross-section. The density and strength are amazing; it took about 30 hits with a hammer to break it, hitting it as hard as I dared without risking being cut (I was holding it by its handle). The whiter flecks are agglomerates of New Zealand kaolin (because of improper mixing of the slurry); later batches were much better.

Knapping Zero4 porcelain


Knapping Zero4 porcelain

This picture has its own page with more detail, click here to see it.

Wikipedia terms Knapping as “the shaping of flint, chert, obsidian, or other conchoidal fracturing stone through the process of lithic reduction to manufacture .. flat-faced stones.” In other words, it is the process of carefully breaking off pieces to create sharp edges and controlled surfaces.

Knapping is a thing. r/Knapping on Reddit has 12k followers. There are lots of YouTube videos, articles and books, websites and even commercial suppliers. Michael Slack has answered the question: Could Zero4 porcelain be knapped? The answer, as you can see, is: Nicely. This is not an arrowhead but a proof of concept biface. Michael was motivated after seeing the glassy internal structure of the fired material. He used 0.3% cobalt, thus the blue color. If you attempt this be advised of the importance of extremely vigorous mixing of the slurry to remove all agglomerates. Try various temperatures to find the most knappable material.

Zero4 porcelain mugs using New Zealand and Grolleg Kaolins


Zero4 porcelain mugs

This picture has its own page with more detail, click here to see it.

Both of these Zero4 fritware porcelain mugs were bisque fired at 1450F and glaze fired at cone 04. The Grolleg version of the porcelain is burning a much pinker color (both the bare body and under our G1916Q3 glaze). In typical feldspar porcelains the color difference between these two kaolins is not nearly so much but here the extra glass development is likely amplifying the presence of even just a little more iron oxide.

Here is what happens when Zero4 porcelain gets lit up


This picture has its own page with more detail, click here to see it.

Wall thickness is 2.5mm. Fired at cone 04. At cone 02 it is much more translucent than this and still stable.

Zero4 translucency at cone 04 and 02


This picture has its own page with more detail, click here to see it.

Wall thickness is about 2.5mm. Although not as clear in the photo, at cone 02 it transmits light much better, the most translucent of any porcelain we have seen. The grainy surface on the piece on the left is because I did not properly mix the slip to remove all the agglomerates of New Zealand kaolin.

Blue and orange stains in Zero4 porcelain fired at cone 06


Blue and orange fritware samples

This picture has its own page with more detail, click here to see it.

Mason 6315 zirconium vanadium blue 1-10% and Mason 6028 Orange 1-10%. In both cases, 6% appears to achieve maximum color (colors will be even brighter when fired to the full cone 04). Both of these are listed as candidates for staining bodies on the reference guide at masoncolor.com. Fritware bodies like this have much more glass development during firing than porcelains and thus amplify stain colors better. It is typical to only use body stains for this type of experiment, but because the firing temperature is so low and firings can be done quickly it is likely that more stains will work that in typical cone 6 or 10 porcelains. This is potentially a good process for jewelry making. Photo courtesy of Karen Ho Fatt Lee.

This is what Zero4 does when I smash a piece with a hammer


This picture has its own page with more detail, click here to see it.

This has happened on multiple occasions; the handle survives holding separate pieces of the remaining mug. The porcelain seems to have an elasticity that enables it to withstand impacts. And it breaks to razor-sharp edges. While this is technically not a mullite porcelain, most people handling and using the ware would not notice.

Inbound Photo Links


Zero4 mugs ready to dry
Zero4 mugs ready for drying


Cone 10R porcelain (left) vs cone 03 porcelain (right)

Links

Glossary Zero3
The designation for a group recipes for body, glaze and engobe (by Tony Hansen), that potters can use to make low fire stoneware and fritware porcelain at 1100C (2000F) or cone 03.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy