0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Rate | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition During Ceramic Firing | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | DTA Test | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | LAS Body | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | LOI-Adjust | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Interaction | Oxide Molecular Formula | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | TGA Test | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Molecular Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Fritware

A porcelain with significant added frit. The frit matures it at a far lower temperature than typical. The strength mechanism is one of particle glass bonding rather than mullite development.

Key phrases linking here: fritware - Learn more

Details

Zero3 fritware compared to a cone 6 non-translucent porcelain.

”Fritware”, in the modern pottery sense, is the crow-bar method of making porcelain vitrify at very low temperatures. Potters typically do it using a frit-for-feldspar (or frit-for-part-of-the-feldspar) substitute in the recipe. Of course, frits are dramatically more expensive than other typical body materials, but their use can bring equally dramatic results. Bodies can be made to fire glassy, white, translucent and super-strong cone 04 (better than seems theoretically possible because there is no development of mullite or anorthite). Fritware porcelains achieve greater density than is possible in traditional porcelains - that density can produce significant strength. However, a downside is the higher firing shrinkage, which in turn will mean more warping on vulnerable shapes. Fritware bodies can be fired at a rapid rate of rise and fall. The extra expense of the frit justifies the use of whiter, more expensive kaolins (and super-white bentonites and smectites), enabling very white fired surfaces. Fritware bodies respond exceptionally well to stains; the glass development intensifies the color.

Blue and orange stains in Zero4 porcelain fired at cone 06.

Traditional porcelains are made from feldspar, clay and quartz, and they fire above 2200F (1065C). Typically, around 20-30% quartz is needed so that common commercial glazes fit. 25-35% feldspar is needed for maturity. The remainder of the recipe is a mix of kaolins, plasticizers and binders (proportions dependent on the amount of plasticity and dry strength needed). As noted, dense and strong fritware bodies at and above cone 04 are most easily formulated by simply replacing the feldspar with a high sodium frit (in North America the most common is Ferro Frit 3110). If lower expansion glazes are available, the percentage of silica can be reduced in favor of more frit (for lower firing) or more clay (for better workability). Fired maturity can be sacrificed if translucency is not needed; this greatly reduces firing shrinkage.

Where plasticity can be sacrificed, or augmented by binders, frit percentages can be increased to 90% or more in the recipe to get a vitreous body as low as cone 020! Using Veegum, such bodies can be plastic enough for forming and throwing. Using binders, even higher frit percentages can be tolerated for casting or pressing.

An advantage of fritware to potters is that standard low-temperature glazes can be used. This includes underglazes. Low-fire transparent glazes produce ultra-clear and brilliant surfaces not possible at higher temperatures. The edges of underglaze decoration also bleed much less. Of course, fritware must be bisque-fired at much lower temperatures (e.g. 1500-1600F or lower) to be absorbent enough for traditional porous-bisque glazing.

If you wish to experiment with fritware, consider mixing our Zero3 or Zero4 porcelains (and matching glazes).

Related Information

Zero4 fritware mugs fired at cone 04


Two porcelain hashtag mugs

This picture has its own page with more detail, click here to see it.

To a potter, it may seem impossible that a body can be this porcelain-like at such a low temperature. And that such a body can be as plastic as this is. Achieving these came at the cost of shrinkage, both drying and firing, 18% total (vs 14% of a Grolleg cone 10 porcelain). Using this Zero4 fritware, very thin-walled pieces can be thrown. The frit also produces a body having a higher thermal expansion, so it fits any low-temperature glaze we have tried. This glaze is G1916QL3 ultra gloss clear glaze on Amaco Velvet underglazes. The low temperature has another benefit: Very sharp edges on painted underglaze designs. Zero4 replaces my old Zero3 fritware with a body that works at a more common temperature. It also employs a tiny amount of blue stain to produce the bluish-white color. Like Zero3, you can also make this yourself.

Zero4 porcelain cup cross-section


This picture has its own page with more detail, click here to see it.

The fritware body is highly plastic and can be thrown very thin. At cone 04, this thin-walled mug did not warp even though it fired to a near-glasslike cross-section. The density and strength are amazing; it took about 30 hits with a hammer to break it, hitting it as hard as I dared without risking being cut (I was holding it by its handle). The whiter flecks are agglomerates of New Zealand kaolin (because of improper mixing of the slurry); later batches were much better.

Zero4 fritware is more resistant to overfiring than you might think


Fritware cast square vessel

This picture has its own page with more detail, click here to see it.

Most technical sources would say that one of the disadvantages of fritware bodies is volatility in firing. They should deform and warp more readily as they reach maturity. And if overfired, we would expect a rapid increase in deformation. However, that is not the experience we have had with Zero4 low fire porcelain. It reaches zero water absorption (maximum density by cone 06, 1800F). Yet it is still very stable at cone 04, which is more than 100F hotter. Also, at cone 04 it achieves very good translucency. But this cast piece, which is about 10 cm tall (4 in) has a wall thickness of only 2.5mm, has wide flat areas that have not warped and it is fired another 100F hotter (cone 02). Yet it is not warping! This body has the same density and firing shrinkage across the entire cone 06-02 range.

Firing a porcelain in less than 4 hours total


This picture has its own page with more detail, click here to see it.

This porcelain mug put into kiln at 8:45am and I was drinking coffee from it at 12:15! How? One way to fast-fire is to fire a lot lower. This is Zero3 porcelain made using Dragonite Halloysite (not quite as white-burning as New Zealand Halloysite). It is the L2934C recipe. It was fired to cone 03 and glazed with G2931K clear glaze (which has fired crystal clear and flawless). I fired at 1200F/hr to 1950F, held it for 15 minutes, cooled at 999F/hr to 1850F and held it for 30 minutes, then dropped as fast as the kiln would do. Is this really porcelain? Yes. And it is super strong. The frit in the recipe is magic, making it vitrify quickly and completely.

Casting Zero3 Porcelain


This picture has its own page with more detail, click here to see it.

Look at how translucent this is! I can fire one of these in three hours, cold-to-cold. I am casting them with molds made using the 3D-printing process. Anyone could do this. Incredibly exciting. And with the G3879 glaze it looks awesome, just like bone china. Notwithstanding this, the Zero3 recipe has to be altered for casting. Initially I have reduced the VeeGum to 1% but it is still casting too slow. And it is not shrinking enough to pull away from the mold well. I am considering strategies on how to increase drying shrinkage and am going to add more frit to take it down to cone 04.

Zero3 casting porcelain at cone 04, 03


This picture has its own page with more detail, click here to see it.

Compared to a typical cone 6 porcelain, left, which has zero translucency, these are fired 10 cones lower. I am using the G3879 clear glaze and it is working very well.

Links

URLs https://en.wikipedia.org/wiki/Fritware
Fritware at Wikipedia
This page has a number of errors to be aware of. Glaze are not applied to harden objects, fritware is hard without them. Tin glazing is not needed for whiteness, it is just as white as porcelains. The frit used is not "crushed silica". It is not innovative because of body and glaze made of the same materials, it is innovative because frit is added to the body. A recipe of "10 parts silica to 1 part glass frit and 1 part clay" is impossible.
Glossary Bone China
A ceramic whose priorities are translucency, whiteness, fired strength and resistance to thermal shock failure.
Glossary Zero3
The designation for a group recipes for body, glaze and engobe (by Tony Hansen), that potters can use to make low fire stoneware and fritware porcelain at 1100C (2000F) or cone 03.
Materials Ferro Frit 3110
High sodium, high thermal expansion low boron frit. A super-feldspar in clay bodies. Melts at very low temperatures. Useful to make crackle glazes.
Materials Veegum
A clay of incredibly small particle size. It has the highest plasticity of any known clay and acts as a suspending and gelling agent in slurries.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy