0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Rate | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition During Ceramic Firing | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | DTA Test | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | LAS Body | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | LOI-Adjust | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Interaction | Oxide Molecular Formula | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | TGA Test | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Molecular Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Clay Stiffness

In ceramics, clays exhibit plasticity in accordance with their recipe but also the water content. Each types of forming method has an ideal combination of stiffness and plasticity.

Key phrases linking here: clay stiffness - Learn more

Details

Clay bodies used in machine forming must have a correct stiffness in order to optimize the forming process. Great effort is expended in the body mixing departments of factories to produce a product of standard stiffness and plasticity. Some processes (e.g. pressing) require clay that is so stiff a potter would need a hammer to move it. Others need clay that is so soft it can be scooped by hand (like cream cheese). Since the body is used soon after it is made, there is no need to worry about how the stiffness might change over time. However, companies that manufacture and sell prepared bodies (either for use in large-scale production or by potters) must carefully consider stiffness. This is because wet (or mud) bodies normally stiffen over time (very important if they won't be used for months or even years). Some bodies can soften during storage; this can happen for a range of reasons (e.g. slight solubility in one or more materials, the presence of electrolytes in the water, particle agglomeration, improper particle surface wetting during mixing), then stiffen.

In addition, it is common for bodies to appear to stiffen, but re-soften as soon as they are wedged or moved. Each body has its own specific water content percentages that correspond to specific stiffnesses. Plasticity variation is the main factor. Usually, the more plastic it is, the more water is needed for a target stiffness. The percentage of water needed for a given stiffness can vary (for the above-mentioned reasons and more), so when deciding how to run a body, production departments may put more weight on the feel of the material leaving the pugmill and use the water content as a secondary guide. Other producers, especially those who tightly control water pH, ball mill and filter press, have greater confidence that 24% water, for example, will always be the right stiffness.

Although there are a variety of devices employed to gauge stiffness, the usefulness of these is often questioned by experienced people (who prefer simply judging by feel).

Cracking problems with drying rise exponentially as the water content of pugged clay rises. So it is better to avoid softer clay unless you have experience using it for the intended application (e.g. with jiggering, the mold quickly pulls water). Using very soft clay on a potters wheel means not being able to throw as thin, as high or as true as would otherwise be possible. More trimming as leather hard will be needed.

The stiffness of clay bodies is sometimes the key enabler for the kind of ware that is made from them. Yixing teapots, for example, are not so much hand-built as they are assembled from precut geometric shapes. The very stiff clay must be flattened with a mallet to make the slabs.
That inconvenience pays off because the stiff clay holds its shape despite being used to make very thin-walled pieces. On the other extreme, clay of paste-consistency is used in 3D printing. And in the making of tandoori ovens, where it is mixed with all manner of fibrous materials to give it strength. And in throwing of gigantic pots in China (where many muscle bound potters throw a piece together).

Production departments benefit when they consider the plasticity of the clay as well as the stiffness. It may be that production issues (e.g. drying cracks, forming splits) are because the clay is not plastic enough, not because it is too stiff.

If you are a hobby potter and a clay has become too stiff (because of water loss) it can likely be softened (assuming the slugs are in plastic bags). Two methods are common.
-Make some small holes on one side of the bag and set it face down on some gravel in the bottom of a water-filled basin (enough water to go a little above the gravel level). If needed, make holes on the other side(s) and put them face down for continued softening.
-Pour the amount of water needed for a slug (e.g. 1 cup) into the plastic bag and tie it. Then immerse the bag in a 5-gallon bucket of water (filled high enough to exert pressure from all sides).
After a few days it should begin to soften.

If clay has become too soft, take the slug out of the bag and wrap it with cloths for a day or two.

You will, of course, need to wedge the clay well to prepare it for use.

Related Information

Is the clay too stiff to use? Maybe not.


This picture has its own page with more detail, click here to see it.

Clays of very high plasticity often stiffen during storage in the bag. This is Plainsman Polar Ice, it contains 4% VeeGum. This slug is like a brick, yet it will loosen up completely. But it is far too stiff to attempt wedging. However, simply throwing it on the floor a few times (turning it each time) will pre-soften it enough to be able to wedge. Then, before you know it, it is too soft and needs to be put on a plaster table to stiffen it before throwing.

This simple device continuously gauges clay stiffness


This picture has its own page with more detail, click here to see it.

Here is how the pugmill operators at Plainsman Clays gauge the stiffness of the clay coming out of the pugmill. The machined nylon roller is on a slant and weighted. The softer the clay the more lines show. When they are like this (5th line steady) the operator knows the water content is around 22% for this clay, Polar Ice. For each type of clays it is different. Stiffness at pugging must also compensate when the clay tends to stiffen or soften over time. Over the years they have tried many devices to measure stiffness, but this has proven the most reliable.

What causes a clay to split like this?


Splitting during throwing

This picture has its own page with more detail, click here to see it.

This is M340, it is not made from a mixture of 200 mesh refined minerals and ball clays, rather, from minimally processed natural mined clay. It is ground at 42 mesh, so the material contains a wide range of particle sizes. Potters who have only used this type of body are at home with it. Its advantages include excellent dry strength, pleasant texture, natural fired character, easy glaze fit and low cost. But downsides are lower plasticity, higher drying shrinkage and splitting. But a case this bad is not normal, it only happens when there is a "perfect storm" of factors:

The best way to prevent this from ever happening is to do the opposite of all the factors just mentioned.

A home made moisture sensor for pugged clay


This picture has its own page with more detail, click here to see it.

This is an Arduino controller board that has been wired to a display and a moisture sensor probe (which is stuck into a piece of soft clay). The sensor outputs a voltage that varies with changes in the resistance encountered between the probes (according to the material being measured). In this case the controller is directly outputting the number being returned by the probe. A study is needed to compare outputs with actual measured water content, this data would enable changing the software to output the percentage-of-water directly. However this sensor is intended for soils, it is not giving repeatability and consistency for measuring the much higher water content found in pugged clay. So we need to find a better one.

Inbound Photo Links



Joining rules are different When clay is soft and plastic

Links

URLs https://www.instagram.com/reel/DTso5owEpf8
Chinese potters team-throwing gigantic porcelain vases
Also making sections and gluing them together with slip at the almost-dry stage. They throw thick walls and do a lot of trimming at the almost-dry stage.
Glossary Plasticity
Plasticity (in ceramics) is a property exhibited by soft clay. Force exerted effects a change in shape and the clay exhibits no tendency to return to the old shape. Elasticity is the opposite.
Glossary Water Content

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy