0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Rate | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition During Ceramic Firing | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | DTA Test | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | LAS Body | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | LOI-Adjust | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Interaction | Oxide Molecular Formula | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | TGA Test | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Molecular Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Code Numbering

In a ceramics lab, studio or classroom specimens of hundreds of glazes and bodies may be present. A code numbering system that links these to written or computer records is essential.

Key phrases linking here: code numbering, code-numbering, code numbered, code numbers, code number, code-number - Learn more

Details

In the context of this site the term "code numbered" means that a recipe record has been created in an insight-live.com account and that record has been assigned a unique code number. This is analogous to the unique ID number that typical LIMS (lab notebook) systems assign for new tests. We do not imply meaning in any but the first alphabetic digits of code numbers we make, they simply need to be unique numbers for unambiguous connections with records in the database.

Labs and studios are typically full of hundreds or even thousands of fired test specimens and their source batches (in jars, bags, pails, etc). When these are uniquely identified with code numbers, they have permanent informational value and a place in Insight-live where information about them can be updated. Moreover, each of those records can be a starting point from which more testing work and development can be done.

Code numbers written on test pieces cross-reference them with computer records

Even when fired specimens are photographed and discarded, their code numbers continue to be the link between written records and the pictures and data. And as labels for buckets, bags, boxes, reference samples, etc. And for searching within Insight-live.

Insight-live recommends a code number of format XNNNN, where the prefix "X" indicates the type of test (as configured in your preferences). Prefixes can be configured to separate different types of testing (e.g. lab tests, production mixes, glaze tests, etc.). NNNN is a sequential number that Insight-live can increment for each new record added. There is a benefit to using four digits, using leading zeros for numbers less than 1000: The code numbers sort in order. G0002 sorts before G1000, but G2 sorts after G1000. Sort order is very important; you always want the most recently added recipe at the top of the list.

Insight-live's assign-next function will tolerate some variation in code numbering as follows:

If the code number of the last-added recipe is non-standard, e.g. P1234-100, Insight-live cannot automatically increment it to assign to the next one added (you will have to manually enter it.

Related Information

Is this your testing records for glaze development?

Lost in binders or buried on your phone


A messy binder that someone uses to store their glaze recipes

This picture has its own page with more detail, click here to see it.

Consider how valuable your glaze and body development records are. Are they in a three-ring binder? Or do you have pictures and notes scattered across apps on your phone? If you're testing, adjusting, or developing glazes, bodies, underglazes or engobes, traditional notebooks and binders are holding you back. They don't have keywords, and they are only grouped, not categorized. With Insight-live, you can link recipes to each other and to important details like photos, materials, firing schedules and URLs. Organize test recipes into projects, classify them with typecodes (tokens), calculate chemistry, and create mix tickets. Research materials and perform keyword searches. Put anything side-by-side to study and determine the next move. Physical notebooks can’t do this—but your account at Insight-live.com can!

Code numbers are the key to organizing your studio or lab


This picture has its own page with more detail, click here to see it.

The new ceramics is about data! Everything here has a code number (in the form x1234) that members of our team can search in our group account at Insight-live.com. We write the numbers on the bottoms of pots, plastic bags of powders/liquids/pugged, buckets, glaze balls, mix tickets, test bars, tiles, glaze samples, drying tests, flow tests, sieve analyses, LOI/water content tests, etc. Glazed fired pieces can have up to three numbers, the body, engobe and glaze. If something is lacking a number it goes in the garbage because it teaches nothing and is therefore taking up pointless space.

Preparing clay test bars to measure plastic, dry and fired physical properties


Preparing bars for the SHAB, LOI and DFAC tests

This picture has its own page with more detail, click here to see it.

This is being done for SHAB, LOI and DFAC tests. The clay was wedged thoroughly, rolled to 3/8 thickness (using the metal rods as gauges) and then cut to 4 1/4" by 1" bars. Code numbers and specimen numbers are stamped on each (these are needed to enter data into our account at Insight-live). For example, notice that the bars have specimen numbers from 1 to 6. These will be fired at six different temperatures (for a low-temperature body, for example, we fire cone 06, 04, 03, 02, 01, 1, 2). The data measured from each, including the temperature, will be entered for each bar (specimen). The 12cm dia. disk is being cut from 3/16" thickness. Notice how these clay tears as cut, this is an indication of the low plasticity of this native clay material. And notice the greenish color, that is typical of terra cotta clays.

A code on every ceramic test:

The link between your samples and your records


Two code-number ceramic mugs

This picture has its own page with more detail, click here to see it.

A promising test is frustratingly difficult to repeat if you cannot identify how you made it. A code number on each specimen links it to its recipe, firing schedule, pictures and notes—and to earlier and later versions in the same project. These mugs and the test bar are made from the same experimental material (called “Battle Clay”). Their code connects them to the records for that test mix. Pretty much everything I have ever made has been a test, and thus has code numbers on the bottoms. I can pick up a 40-year old specimen and find its history, or open the record and locate the matching pieces (in my Insight-live.com account).

Throwing a clay body is an invaluable physical test

But pieces need to be code numbered for tracking


This picture has its own page with more detail, click here to see it.

Throwing a clay on a potters wheel gives immediate feedback on the physical properties (e.g. texture, plasticity, degree of softness, tendency to split, etc). A fancy report full of numbers gathered from expensive testing equipment takes a lot more time and is not likely to be as valuable as this. If you are doing testing, and everyone should be testing body and glaze variations, then all tests need to be identified. Do that with a code number that cross-references into your account at Insight-live.com.

Stamp used for stamping information onto clay test bars


12 digit rolling stamp

This picture has its own page with more detail, click here to see it.

Code numbering is an essential part of any testing program. This type of stamp is ideal for stamping code numbers and other information on plastic clay test specimens (e.g. SHAB test bars). Set up the run or recipe number on the left and the specimen number on the right. You can find these stamps on Amazon by searching "12 digit rolling alphabet symbol number stamp".

Every studio, lab, classroom needs a good label printer


This picture has its own page with more detail, click here to see it.

This is an Epson LW-600P (replaced by the LW-PX400 in 2021, but still available on eBay). It generates durable water-proof labels that are perfect for identifying buckets and jars of materials and glazes. Apps are available for iOS, Android, Windows and Mac. You can insert a QRCode on to a label (perfect for taking someone to an SDS or information page). Insight-live emphasizes assigning unique code numbers to all recipes you create and maintain, this is the perfect way to prominently display it. We find the yellow 18mm labels work well to display code numbers (the white 22mm for detail). The cartridges snap in in seconds so it is easy to change them. While the printer does support blue-tooth, enabling anyone with a phone to use the device, for routine label-making it works best when USB-connected on a desktop computer (the app works better and there is no waiting).

Here's how we used to record test results before insight-live.com


An example of how a potter presents side by side glaze recipe tests

This picture has its own page with more detail, click here to see it.

Side-by-side presentation. That’s the best. But I magine if you could put, side by side; the recipes, pictures, notes, data, of any recipe test you had ever done. Even results of testing you did on commercial prepared glazes and glaze combinations. And be able to link, search, print, share them. That’s what you do in Insight-live. Pottery has always been about the data, we just let that information die before! Now we can learn so much more from it. Photo courtesy of Brielle Rovito, Burlington, Vermont, USA.

Inbound Photo Links



John Porter’s fired glaze samples are being catalogued

Links

Glossary Digitalfire Insight-Live
A cloud-hosted ceramics-targeted LIMS (lab info management system). It does glaze chemistry and physical testing the “Digitalfire way”. For technicians, educators, potters and hobbyists.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy