0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Rate | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition During Ceramic Firing | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | DTA Test | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | LAS Body | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | LOI-Adjust | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Interaction | Oxide Molecular Formula | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | TGA Test | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Molecular Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Throwing

The process of forming soft clay on a potter's wheel.

Key phrases linking here: throwing, thrown - Learn more

Details

Vase thrown on potters wheel
Made from Plainsman M390 clay.


Throwing is a forming process in ceramics, it has been synonymous with pottery for millenniums. It is magic to watch and looks easy, but it is not. A lot of determination is needed to learn this skill and it is one that is never mastered completely, improvement never stops for those who seek it. Each potter has his own style, there is no "right way". Each type of object has its own throwing challenges, the most dedicated throwers will make thousands of just one type of piece to perfect it.

Plastic clay is said to "throw well". Throwing is actually one of the best tests of plasticity (since there is no reliable instrument that can measure this property). Simply taking two pieces of clay of the same weight and throwing the largest thinnest vessel possible of each compares their plasticities.

Traditional potters like this in Japan or Korea used (and use) non-plastic clays, aging them to at least optimize it as much as possible. It can appear that they throw impossibly large thin-walled pieces out of very soft clay, but the laws of physics apply to them like anyone else, pieces are thicker walled than they appear. But they do teach us much account listening to the clay and working patiently and methodically.

Modern pottery clays and porcelains, especially in the west, incorporate ball clays and bentonite to have as much plasticity as needed, this makes them very easy to throw even by beginners. Most people these days learn on Youtube, thousands of videos are likely available. If you are just starting it can be helpful to follow some simple guidelines:

-Don't use the clay too soft
-Don't hurry, movements to center, lift and shape should be slow and deliberate
-Don't release pressure quickly, let go slowly
-Squeezing the clay wall does not lift it, one of your hands or fingers has to get under the clay to lift it
-Your hands should be touching each other whenever possible to be more steady
-Grogged clay increases friction between the clay and your fingers, avoid it (if pieces are dried evenly no cracks will happen)
-Keep the inside and outside angle between base and wall as square as possible so that all lifts have a good start
-Learn the right speed
-Learn to use the right mix of slip and water to lubricate well at all times
-When centering the clay, push away and pull toward yourself (rather than press laterally from each side)
-Minimize the area of contact between your hands and the clay when centering (by cupping them), this increases the pressure and moves the clay better
-Avoid to many fancy tools at the start, but make sure you have a good sponge and rubber rib
-Be prepared to lose lots of pieces, just start with another piece of clay when you run into trouble.

Related Information

Throwing a pot on a potters wheel


This picture has its own page with more detail, click here to see it.

Throwing a Polar Ice mug on the potter's wheel

Polar Ice is plastic enough to be able to throw mugs having walls as little as 3mm thick (bottom-to-top). It is very sticky if too soft so I stiffen it on a plaster table before throwing it. The video is speeded up in the middle section.

Birds-eye-view throwing a terra cotta mug

The video is speeded up in the middle portion. I am wearing camera glasses so please forgive the jerkiness and off centre of the video. This type of clay body is normally very plastic, better throwers must consciously be careful not to make walls too thin.

Why throw on a plaster bat when making larger pieces?


A large thrown vessel, having dried overnight under plastic and on a plaster bat, is ready to turn o

This picture has its own page with more detail, click here to see it.

To achieve more even drying. As soon as was practical after throwing (a few hours), I covered the piece with a cloth and then put a garbage bag over it. While that put the upper section a little ahead of the base in drying, over night the base caught up (the plaster sucks the water out of it, even the walls of the piece stiffen). In the morning I remove the plastic and within an hour or two it is ready to lift off the bat and turn over, shortly after that I can trim it. I secure each plaster bat to the wheel-head using a "Batmate", that works extremely well. To stick the clay to the plaster well I apply a thin layer of slip, round off the piece of clay and firmly slam it down onto the plaster (if it is not rounded it will not stick as well or may break the bat). This is quick and effective to achieve the even drying needed to avoid a drying crack. This method is especially important for large plates and bowls, which often suffer s-cracks.

Why do some clays split like this on throwing or forming?


A split on the lip of a bowl

This picture has its own page with more detail, click here to see it.

An example of splitting, where a clay develops a split minutes after throwing. This often happens at stretch-points with sandy or groggy or minimally processed natural bodies that have a wide range of particle sizes (e.g. native bodies). When larger particles are poorly bonded by fine plastic clays, they can form networks into which water can penetrate. This issue is referred to as "splitting" because it is progressive, a crack starts, and it grows over a period of minutes. If you use bodies susceptible to this issue, various habits can be formed to minimize this problem. Perhaps the most important is not to leave water or high-water-content slip on any surfaces experiencing tensile stress (e.g. flared bowls, bellied vases).

Tobla Howell throwing Plainsman raku clay.


This picture has its own page with more detail, click here to see it.

Links

Glossary Slip Casting
A method of forming ceramics. A deflocculated (low water content) slurry is poured into absorbent plaster molds. As it sits in the mold, usually 10+ minutes, a layer builds against the mold walls. When thick enough the mold is drained.
Glossary Casting-Jiggering
A process in ceramic production where items are slip-cast first and then finished using a jigger wheel.
Glossary Jiggering
Jiggering is a process of forming pottery that employs a spinning plaster mold and a tapered template to press soft clay or porcelain against it.
Glossary Hot Pressing
Glossary Dust Pressing
Many ceramic products, especially tile, are formed by pressing high-moisture or binder-containing dust or pelletized dust into steel molds at high pressures.
URLs https://www.instagram.com/reel/DTso5owEpf8
Chinese potters team-throwing gigantic porcelain vases
Also making sections and gluing them together with slip at the almost-dry stage. They throw thick walls and do a lot of trimming at the almost-dry stage.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy