0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Rate | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition During Ceramic Firing | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | DTA Test | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | LAS Body | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | LOI-Adjust | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Interaction | Oxide Molecular Formula | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | TGA Test | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Molecular Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Cordierite Ceramics

Cordierite is a man-made refractory low thermal expansion crystalline solid that forms at very high temperatures (in the right mix of kaolin and talc).

Key phrases linking here: cordierite ceramics - Learn more

Details

Cordierite ceramics are well known for their low thermal expansion and refractory character. Although cordierite is available as a powder, here we are generally talking about ceramic that went into the kiln as an ordinary composite of mineral powders but emerges as a solid cordierite crystalline matrix (grown by the firing process tuned to its needs).

Cordierite makes the ceramic manufacture of products like catalytic converters possible. Barrett’s Minerals, near Dillon, MT, claims to make the talc used in making the converters for all cars in North America. They constantly heat up and cool down quickly and must not crack because of the shock. These converters get their thermal shock resistance properties from a bonded matrix of low-expansion cordierite crystals.

Cordierite crystals form during firing between 1200-1400C (~cone 6-15). Interestingly, cordierite crystals have a lesser thermal expansion along one axis than another. The ideal chemistry to produce the crystals is 13.8% MgO, 34.8% Al2O3 and 51.4% SiO2 (2MgO, 2Al2O3, 5SiO2). Talc, kaolin and raw alumina powder can be blended to source this chemistry (other materials are also used e.g. aluminum hydroxide, steatite and other MgO minerals). Multiple factors determine the temperature and extent to which cordierite develops. Materials sourcing more than one oxide (like kaolin and talc) may react better than pure oxide materials (like MgO, Al2O3, SiO2). Materials of finer particle size react better. Better cordierite development occurs when the precursor mix is pressed to higher densities and firing schedules are tuned (in rate-of-climb, ultimate temperature and holding patterns). Thermal expansion measuring equipment is needed to study the relationships between materials, process and firing on the quality of cordierite produced. As noted, the ultimate goal is the development of a continuous crystal matrix of cordierite (not just the presence of the crystals in an otherwise typical ceramic).

Lacking testing equipment a potter can produce cordierite to some extent, and therefore make ware having greater resistance to thermal shock failure. A simple firing of a body having the above recipe to cone 10 or 11 and held should produce some crystal development. There is also a more direct approach: Cordierite powder is available, it is prefired and finely ground. It can be plasticized for forming and bonded during firing (at much lower than normal cordierite creation temperatures) to produce a ceramic with lower expansion.

Cordierite is very practical as a refractory for kilns shelves and kilns posts because of its combination of low cost and low thermal expansion. Of course, it is not as refractory as alumina or SiC so is generally suitable for light duty use.

While cordierite ceramic vessels could be made (e.g. ovenware), the material has such a low thermal expansion it is very difficult (or impossible for most technicians) to match a glaze (without crazing). Notwithstanding this, many recipes can be found for cordierite ovenware or flameware. However, these are seldom fired above cone 10 so any thermal shock resisting behavior they have is attributable to grog content or their open fired matrix rather than to any cordierite development.

Related Information

An electric kiln half shelf that costs $500!


This picture has its own page with more detail, click here to see it.

This Advancer Nitride-bonded Silicon Carbide shelf is 26 inches wide (by 1/4 inch thick) weighs 9 lbs. These are incredible durable and strong. However there are cautions to their use. They can act as an electrical conductor so must not contact elements and should not be used in kilns with unpinned elements protruding from grooves. They must be stored in a dry place to prevent moisture penetration (which can cause a steam explosion during heatup). The company has a recommend drying schedule if shelves do absorb moisture (the application of kiln wash is not considered a prolonged exposure and is OK).

Links

Materials Talc
A source of MgO for ceramic glazes, a flux or thermal expansion additive in clay bodies, also used in the manufacture of cordierite.
Glossary Thermal Expansion in Ceramic Bodies and Glazes
The co-efficient of thermal expansion of ceramic bodies and glazes determines how well they fit each other and their ability to survive sudden heating and cooling without cracking.
Glossary Refractory
In the ceramic industry, refractory materials are those that can withstand a high temperature without deforming or melting. Or can be sintered into super materials.
Glossary Flameware
Flameware is ceramic that can withstand sudden temperature changes without cracking. The low thermal expansion of true flameware makes craze-free glazes very difficult.
Glossary Crucible
In ceramics, potters make crucibles to melt frits, stains and other materials. Crucibles are made from refractory materials that are stable against the material being melted in them.
Glossary Ceramics
This term generally refers to the industry that produces the non-metallic objects we use every day (like porcelain, tile, glass, stoneware).
Glossary Ovenware
Ovenware clay bodies have a low expansion by virtue of materials in their recipe and/or the way they are fired. But potters bend the rules.
URLs http://en.wikipedia.org/wiki/Cordierite
Cordierite at Wikipedia
URLs http://www.ceramicindustry.com/articles/85334-materials-synthesizing-cordierite-in-ceramic-bodies
Ceramic Industry article on synthesizing cordierite
URLs https://www.dieselnet.com/tech/cat_subs_cer.php
How catalytic converter cordierte substrates are made
URLs https://www.tilemachinery.com
Xiangtan Weida Electrical and Machinery Co., Ltd
They make feeders, crushers and grinders, Raymond mills, ball mills and filter presses, mixers, pug mills, cutting machines, forming presses, setting machines, kilns and dryers. Also production lines for cordierite catalysts, clay roofing, terra cotta facades, tile and ceramic rollers.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy