0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Case Mold | Casting Rate | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition During Ceramic Firing | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | DTA Test | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | LAS Body | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | LOI-Adjust | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Interaction | Oxide Molecular Formula | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | TGA Test | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Molecular Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Water in Ceramics

Water is the most important ceramic material, it is present every body, glaze or engobe and either the enabler or a participant in almost every ceramic process and phenomena.

Key phrases linking here: water in ceramics - Learn more

Details

There is a need to discuss water in ceramic production as it related to a number of natural phenomena and production processes:

Plasticity: Clays are plastic because water glues and lubricates the particles. The micro-dynamics of this are complex.

Rheology: Suspensions (solids:water systems) exhibit properties (like viscosity, thixotropy) that are a product of the way particles interact with the water, each other and the way electrolytes affect the system.

Solubility: Generally, in traditional ceramics, insoluble materials are employed to make body and glaze slurries. However, in actual practice, many materials are slightly soluble over time and thus introduce electrolytes that affect the pH in a linear or non-linear fashion (and therefore rheological properties) of the system. Solubility is much less of an issue when the water:solids mix is not stored (used immediately).

Particle surface area, surface charge and size: Almost all glazes and bodies contain 'live' particles (like clay) that interact with water. The degree to which they interact and the total surface area that does that interaction profoundly affects the physical properties and the amount of water needed.

Dehydration and Decomposition: Many minerals are hydrates and thus have water bound in the crystal structure itself. This has to be ejected during firing. For product quality and even survival in the firing, it is important to understand how and when they convert from one phase to another (and release water at each). At times multiples conversions occur as a firing proceeds. In addition, bodies and glazes are mixtures of multiple minerals each having its own dehydration profile.

Dewatering: Many raw materials and even bodies are wet processed for purification purposes and must be dewatered to either powder stage or production use stage (an energy intensive process).

Drying: Water must be removed from bodies in such a way that articles do not crack during drying or explode during firing (due to steam pressure). Even when a piece appears dry it still likely contains 5% or more mechanical water that only drying above its boiling point will remove. The smaller the finest particle sizes the longer it will take to dry and the greater the drying shrinkage will be (some clays may literally need ten times longer to dry than others). Glazes and engobes likewise need to be dried in such a way that they do not crack and they maintain their bond with the body.

Focus on the actual formulations that utilize water is also helpful:

Plastic bodies: Water is the vehicle that makes the clay plastic and the primary focus is having the amount of water needed to get the desired stiffness (typically 17-23%) and seeing that it is incorporated in such a way that all particle surfaces are whetted. Electrolytes enhance or degrade that plasticity immediately and over time (if they they dissolve in the water). In industry, water is typically filtered and processed before being put into bodies to minimize the unknown (and therefore unwanted) electrolytes. Water can also dissolve salts in the body and cause efflorescence during drying.

Glazes: The rheological properties of glaze slurries are a product of the amount of water (typically 40-55%) and the way that water interacts with the inert material particles (like feldspars and quartz), the charged particles (like clays) and the conditioners (like gums, deflocculants, electrolytes). Highly fritted glazes need less water, those with alot of clay (especially fine-particles clay) need more. Water quality is more critical than with bodies because electrolytes have a greater affect on the working presence. In addition, the viscosity and thixotropy of glazes is even more likely to change over time when glazes are stored.

Casting slips: The same as glazes but with a focus on minimizing the quantity of water (to around 25-30%) by introducing electrolytes that deflocculate the slurry while at the same time producing a thixotropy that prevents particle settling. Casting slips are a finely tuned water:solids system whose rheology is even more fragile to change than glazes (when extra and unknown electrolytes are entering it by slowly dissolving from materials in the slurry).

Related Information

Links

Glossary Rheology
In ceramics, this term refers to the flow and gel properties of a glaze or body suspension (made from water and mineral powders, with possible additives, deflocculants, modifiers).
Glossary Deflocculation
Deflocculation is the magic behind the ceramic casting process, it enables slurries having impossibly low water contents and ware having amazingly low drying shrinkage
Glossary Mineralogy
Raw ceramic materials are minerals or mixtures of minerals. By taking the characteristics of these into account technicians can rationalize the application of glaze chemistry.
Glossary Efflorescence
A common problem with dry and fired ceramic. It is evident by the presence of a light or dark colored scum on the dry or fired surface.
Glossary Plasticity
Plasticity (in ceramics) is a property exhibited by soft clay. Force exerted effects a change in shape and the clay exhibits no tendency to return to the old shape. Elasticity is the opposite.
Glossary Surface Area
The surface area of a powder can be measured. It is the total surface area of all the particles in a gram of the material, and this number can be alot larger than you might think.
Glossary Decomposition During Ceramic Firing
How ceramic raw materials decompose during firing, releasing water, carbon dioxide and other gases that can cause bloating, pinholes and glaze defects.
Glossary Suspension
In ceramics, glazes are slurries. They consist of water and undissolved powders kept in suspension by clay particles. You have much more control over the properties than you might think.
Glossary Viscosity
In ceramic slurries (especially casting slips, but also glazes) the degree of fluidity of the suspension is important to its performance.
Glossary Slip Casting
A method of forming ceramics. A deflocculated (low water content) slurry is poured into absorbent plaster molds. As it sits in the mold, usually 10+ minutes, a layer builds against the mold walls. When thick enough the mold is drained.
Glossary Leaching
Ceramic glazes can leach heavy metals into food and drink. This subject is not complex, there are many things anyone can do to deal with this issue
Glossary Water Solubility
The water solubility of ceramic materials is an important consideration to their usability in the process. Glazes are suspensions of insert powders, solubles present problems to this system.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy