Pure clay mineral, there are many brand names of varying purity and iron content.
| Materials |
Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries. |
| Materials |
600 Kaolin
|
| Materials |
A Kaolin
|
| Materials |
Glomax LL Kaolin
|
| Materials |
Ajax P Kaolin
|
| Materials |
Albion Form 100
|
| Materials |
Albion Sperse
|
| Materials |
Allen G Kaolin
|
| Materials |
Avery Kaolin
|
| Materials |
B Kaolin
|
| Materials |
Bell Kaolin
|
| Materials |
Puraflo 50 Kaolin
|
| Materials |
C Kaolin
|
| Materials |
Calcined Kaolin
This is kaolin powder that has been fired in a furnace to remove the 12% crystal water and render it non-plastic. |
| Materials |
CC China Clay
|
| Materials |
CC31 China Clay
|
| Materials |
Ceraclay WTC Kaolin
|
| Materials |
WTD Kaolin
|
| Materials |
CF Kaolin
|
| Materials |
Cyprucast
|
| Materials |
D Kaolin
|
| Materials |
Diamond Kaolin
|
| Materials |
E Kaolin
|
| Materials |
English Kaolin
|
| Materials |
EP Kaolin
A kaolin that gels slurries (good for suspending glazes). It has two variations: a low and medium plasticity. It fires white for use in porcelain bodies. |
| Materials |
Ewing Kaolin
|
| Materials |
F. C. Kaolin
|
| Materials |
Glomax LL Calcined Kaolin
|
| Materials |
Grolleg Kaolin
A white burning kaolin from the UK, commonly used in porcelain bodies and as a glaze suspender. Sticky when wet, low plasticity. |
| Materials |
Gunheath Kaolin
|
| Materials |
Hamilton Kaolin
|
| Materials |
Helmer Kaolin
|
| Materials |
Hillman Kaolin
|
| Materials |
Hong Kong Kaolin
|
| Materials |
IXL 34E
|
| Materials |
IXL 34E/F 95
|
| Materials |
IXL RE
|
| Materials |
JHC White Kaolin
|
| Materials |
K1 Kaolin
|
| Materials |
K50 Kaolin
|
| Materials |
Kamec Kaolin
|
| Materials |
Kampaku Kaolin
|
| Materials |
Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries. |
| Materials |
Kaolin Slurry
|
| Materials |
Kaopaque 20 Kaolin
|
| Materials |
Kaopolite K 129
|
| Materials |
Kingsley Kaolin
|
| Materials |
KMS Kaolin
|
| Materials |
Korean Kaolin
|
| Materials |
KT-Cast Kaolin
|
| Materials |
LG Kaolin
|
| Materials |
LPC Kaolin
|
| Materials |
Mastercast Kaolin
|
| Materials |
Masterfil Kaolin
|
| Materials |
Masterfloat Kaolin
|
| Materials |
McNamee Kaolin
|
| Materials |
Monarch Kaolin
|
| Materials |
No. 50 China Clay
|
| Materials |
NSC Kaolin
|
| Materials |
Peerless 2 Kaolin
|
| Materials |
Pioneer Kaolin
|
| Materials |
Piopot Kaolin
|
| Materials |
Pleyber G
|
| Materials |
Pleyber P
|
| Materials |
Pleyber S Kaolin
|
| Materials |
Putnam Kaolin
|
| Materials |
Putnam S Kaolin
|
| Materials |
Qc China Clay
|
| Materials |
Rampant BB Kaolin
|
| Materials |
Remblend Kaolin
|
| Materials |
Rogers Kaolin
|
| Materials |
SA-1 Kaolin
|
| Materials |
SAF Kaolin
|
| Materials |
Samson Kaolin
|
| Materials |
Sapphire Kaolin
|
| Materials |
Snobrite Kaolin
|
| Materials |
Sparks Kaolin
|
| Materials |
Standard Porcelain Kaolin
|
| Materials |
Stannon Kaolin
|
| Materials |
Tile #6 Kaolin
The most plastic kaolin in North America, most suitable for making plastic porcelains but increasingly being used in glazes to replace EPK. |
| Materials |
Treviscoe Kaolin
|
| Materials |
Plainsman Troy Clay
|
| Materials |
Velvacast Kaolin
|
| Materials |
WC-5 Kaolin
|
| Materials |
Wilclay CR Kaolin
|
| Materials |
Wilclay WC Kaolin
|
| Materials |
Wilson Kaolin
|
| Materials |
WS Kaolin
|
| Materials |
KAOLIN-SERPENTINE
|
| Materials |
Lampang Kaolin
|
| Materials |
Zedlec Kaolin
|
| Materials |
Delta Kaolin
|
| Materials |
Kaolex D-6 Kaolin
|
| Materials |
Laguna #1 Kaolin
|
| Materials |
Snocal 707 Kaolin
|
| Materials |
Grade C Kaolin
|
| Materials |
Sovereign Kaolin
|
| Materials |
Kaolin Natural BP
|
| Materials |
Speswhite Kaolin
|
| Materials |
Super Standard Porcelain
|
| Materials |
Stockalite Kaolin
|
| Materials |
Supreme Kaolin
|
| Materials |
Topaz Kaolin
|
| Materials |
DB Float Kaolin
|
| Materials |
Allen Kaolin
|
| Materials |
James Bay Stn Kaolin
|
| Materials |
JB Kaolin
|
| Materials |
Kaolin 111
|
| Materials |
Kaolin 113
|
| Materials |
Kaolin 114
|
| Materials |
Kaolin 115
|
| Materials |
Kaolin 143
|
| Materials |
Kaolin 151
|
| Materials |
Kaolin 171
|
| Materials |
Quartz 741
|
| Materials |
Quartz 761
|
| Materials |
Quartz 762
|
| Materials |
Flint Pebbles
|
| Materials |
D'Arvor Kaolin
|
| Materials |
Lunday Kaolin
|
| Materials |
Old Mine Kaolin
|
| Materials |
H-1 Kaolin
|
| Materials |
609 Kaolin
|
| Materials |
1431 Kaolin
|
| Materials |
1433 Kaolin
|
| Materials |
1434 Kaolin
|
| Materials |
1479 Kaolin
|
| Materials |
38 Kaolin
|
| Materials |
Klondike Kaolin
|
| Materials |
VC-1 Kaolin
|
| Materials |
A-1 Kaolin
|
| Materials |
Richardsons Kaolin
|
| Materials |
M+M China Kaolin
|
| Materials |
M.G.R. Kaolin
|
| Materials |
M.W.M. Kaolin
|
| Materials |
No. 44 Kaolin
|
| Materials |
No. 17 Kaolin
|
| Materials |
372 Kaolin
|
| Materials |
Dixie Clay
|
| Materials |
Langford Kaolin
|
| Materials |
Bilt-Cote Kaolin
|
| Materials |
PAR Kaolin
|
| Materials |
Peerless 3 Kaolin
|
| Materials |
Sterling Kaolin
|
| Materials |
Kernick Kaolin
|
| Materials |
Calcined Topaz Kaolin
|
| Materials |
Kaolin G1
|
| Materials |
Opeal OP-6 Kaolin
|
| Materials |
KR-LYK-70 KAOLIN
|
| Materials |
Arcano Kaolin
|
| Materials |
Whitemud Kaolin
|
| Materials |
Whitemud Meta Kaolin
|
| Materials |
Burgess Iceberg Calcined Kaolin
|
| Materials |
Kaolin SP
|
| Materials |
Zettlitzer Kaolin
|
| Materials |
Kaolin A
|
| Materials |
Eckalite Kaolin
|
| Materials |
Ferrous Oxide and Calcined Kaolin Eutectic
|
| Materials |
Magnesia and Calcined Kaolin Eutectic
|
| Materials |
Manganous Oxide and Calcined Kaolin Eutectic
|
| Materials |
Caolín Gris (Cuba)
|
| Materials |
Caolín Blanco (Cuba)
|
| Materials |
Caolín Mantua (Cuba)
|
| Materials |
Caolín Damanueco (Cuba)
|
| Materials |
Caolín Santa Elena (Cuba)
|
| Materials |
Kaolin 233
|
| Materials |
OptiKast Kaolin
|
| Materials |
Eckaglass Kaolin
|
| Materials |
Dragonite Halloysite
|
| Materials |
Wilco-UPF Kaolin
|
| Materials |
SKT-1433 Kaolin
|
| Materials |
Spinks Kaolin Low Residue
|
| Materials |
KaoPearl CNL30 Kaolin
|
| Materials |
Ione kaolin
|
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
Buy me a coffee and we can talk