Oct 22, 2026: We are working on protecting our servers against the PHP2Shell vulnerability recently discovered. Servers were upgraded ahead of schedule on Oct 21. This could cause some issues. Please contact us if you encounter any.

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Kaolin 114

Alternate Names: Kaolen 114

Oxide Analysis Formula Tolerance
CaO 0.25% 0.02
MgO 0.24% 0.02
K2O 0.40% 0.02
Na2O 0.38% 0.02
TiO2 0.35% 0.02
Al2O3 26.50% 1.00
SiO2 60.16% 3.85
Fe2O3 0.82% 0.02
LOI 10.90%n/a
SO4 0.71%n/a
Oxide Weight 342.95
Formula Weight 388.00

Notes

Available in run-of-mine, 25mm and 50mm sizes.

Related Information

Links

Minerals Quartz
Quartz is the most abundant mineral on earth, it is the main crystalline mineral form of silica (SiO
Minerals Kaolinite
The most fundamental clay mineral. This mineral is found in nature in its purest form as kaolin. How
Materials Kaolin 151
Materials Kaolin 115
Materials Kaolin 171
Materials Kaolin 143
Materials Kaolin 111
Materials Kaolin 113
Materials Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries.
Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.

Data

Firing Shrinkage 1000C: 7.5% 1100C: 9% 1200C: 9.5% 1250C: 10.5%
Water absorption 1000C: 20.5% 1100C: 19.5% 1200C: 17.7% 1250C: 17%

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved