3DP | | AIF | ABR | | BIN | ADV | AGT | PHY | ASR | ALM | uAz | ALS | E11 | JWK | ART | ARC | EBA | LAG | PBA | BLC | NFi | mQi | BIN | 62N | BIO | BSQ | CHP | BDT | BGD | BGP | BFR | Csu | DZc | BRK | HWi | SCS | MCB | SCB | ECS | CSP | OLC | CRE | CPM | CRS | STN | CST | LBS | TIL | C3D | CBM | CLM | ECM | CLO | SLR | CRT | CCT | CLT | GBG | CCO | CCN | CRP | d3S | CGS | OCS | DEC | DFT | TM2 | | Dux | DRP | DSP | ELE | ELT | SEU | MUE | EEE | MEQ | SCE | EQD | EQP | EQM | EMR | SER | EQS | | ETC | P3D | PAR | PAU | PCA | PBF | PDE | PGL | PKB | PMM | PPO | PPP | PSH | PWT | EXT | FEL | TAA | FRC | 9h6 | FLB | kK5 | FLS | FRT | MFM | YtL | F3D | EGK | GNM | DGE | GBC | GBS | GLS | GLI | GLC | GLM | GLR | GLT | MGL | FGE | GLZ | GEQ | EHE | HMT | h79 | HTR | CHS | Niv | I3D | ICS | IDP | IGR | EAP | ISO | Qno | qhK | KAO | KCD | EKB | KIL | MKL | SKL | LNS | LAB | vLv | FRL | 7hb | LEM | CQL | LTR | MSH | MOF | MAN | | MRK | MDS | MMC | MPC | MTS | MTT | | MAM | MAA | MDE | MTE | EMP | MPE | CLM | DEN | PWH | MAT | e38 | MTR | BDW | PMF | MIN | 3MM | MMK | EMM | MNC | EMF | yPu | NOX | SOC | | DSL | OPA | QKk | OXI | RED | PTT | SWS | PPS | PRP | | SPM | MPB | SPB | FRP | 9Hv | POI | PEN | PTW | PEQ | a87 | WKS | EPR | PRS | PRT | | PRD | PRO | | | | QCC | RMP | RSR | SRM | MRM | MGR | RFR | wWm | REF | EAR | SRS | ESK | SWR | | SCU | | YFh | SIL | ESR | LrD | YnJ | ESP | MSM | Tmx | STC | OLS | k67 | JXh | PWS | TWC | EPW | TCP | TCE | WSN | TLS | MTL | STL | TGR | OTR | | | UNI | UVR | FWK | gLF | WRS | WPS | YQd

A List of Classic Base Glazes for Pottery

These span the range from low to high temperature. Each is a base or a base plus added pigments, variegators and/or opacifier. The glazes are suitable for functional surfaces. It would be common to buy commercial products to enhance non-functional surfaces. These are suggested package sizes for production.

Cone 6 Dipping glazes or base coat dipping glazes in 2 gallon pails (~5000g powder)

G2934 transparent MgO matte (also commonly mixed as a white by adding zircopax)
G1214Z1 transparent Ca matte (common opacified using titanium)
G2926B transparent glossy (also commonly mixed as a white by adding zircopax)
GA6-B Alberta Slip base (honey transparent)
MA6-C Alberta Slip floating blue
GR6-M Ravenscrag floating blue
G3933A Oatmeal silky matte
G2926BL Jet black glossy (commonly mixed as a first coat)
G2934BL Jet black matte (commonly mixed as a first coat)

Black Engobes/Underglazes in 1 litre jars (~800g of powder)

L3954F Black engobe or brushing underglaze for M340 at cone 6
L3954N Black engobe or brushing underglaze for H550 at cone 10R

Cone 10R Dipping glazes in 2 gallon pails (~5000g powder)

G1947U Base transparent glossy
G2571A Dolomite transparent matte
GR10-C Ravenscrag talc silky matte
GR10-A Base Ravenscrag clear

Low Temperature Dipping glazes in 1 gallon pails (~2500g powder)

G1916Q (or variants) Cone 04 transparent base glossy
G3879 (or variants) Cone 06 transparent glossy

Related Information

Brush-on commercial pottery glazes are perfect? Not quite!


This picture has its own page with more detail, click here to see it.

Brushing glazes are great sometimes. But they would be even greater if the recipe was available. Then it would be possible to make it if they decide to discontinue the product. Or if your retailer does not have it. Or to make a dipping glaze version for all the times when that is the better way to apply. The glaze manufacturer did not consider glaze fit with your clay body, if they work well together it is by accident. But if you have transparent and matte base recipes that that work on your clay body then adding stains, variegators and opacifiers is easy. And making a brushing glaze version of any of them. Don't have base recipes??? Let's get started developing them with an account at insight-live.com (and the know-how you will find there)!

Gemini describes a pottery glaze recipe like a salesman


This picture has its own page with more detail, click here to see it.

This is 2026. It uses expressions like "designed for performance", "specifically engineered", "perfectly transparent", "strict limit formulas", "perfect balance", and "ultimate". Really? Doesn't calling a recipe "ultimate" suggest that if one has an issue with it, then the problem is automatically with them, not the recipe? No. Consider:

-Glazes are systems, not recipes. They have many mixing, application, drying, firing, surface and aesthetics properties that interrelate. Add to that cost, material availability and consistency, material solubility, changes with aging and microbial response. These properties all play against each other; if you want one, you have to give up another. You can optimize some of them at the expense of others.
-Non-recipe factors, like firing method and schedule, application methods, body or engobe or slip underneath, and mixing methods, can really affect performance.
-The only recipe that is perfect for you is the one you develop and fine-tune to have the property pluses that favour your priorities and the faults that match what you can tolerate. The expression "perfect balance" thus applies only to Ron Roy who formulated it.

One more reason to become your own glaze engineer.

Links

Articles Concentrate on One Good Glaze
It is better to understand and have control of one good base glaze than be at the mercy of dozens of imported recipes that do not work. There is a lot more to being a good glaze than fired appearance.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved