Description: Cuban kaolin
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 48.30% | 2.38 | |
| Al2O3 | 34.40% | 1.00 | |
| Fe2O3 | 2.10% | 0.04 | |
| TiO2 | 0.48% | 0.02 | |
| CaO | 0.69% | 0.04 | |
| MgO | 1.50% | 0.11 | |
| K2O | 1.90% | 0.06 | |
| Na2O | 0.12% | 0.01 | |
| LOI | 11.10% | n/a | |
| Oxide Weight | 265.35 | ||
| Formula Weight | 298.48 | ||
| Materials |
Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries. |
| Materials |
Arcilla de Pontezuelo (Cuba)
|
| Materials |
Caolín Blanco (Cuba)
|
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |