Opeal OP-6 Kaolin

Description: Super-white ball clay

Oxide Analysis Formula Tolerance
SiO2 47.49% 2.17
Al2O3 37.13% 1.00
Fe2O3 0.22% -
TiO2 0.01% -
CaO 0.11% 0.01
MgO 0.02% -
K2O 1.10% 0.03
Na2O 0.07% -
LOI 13.85%n/a
Oxide Weight 236.66
Formula Weight 274.71

Notes

Super-white polished tiles, tableware, ceramic glaze,etc.

Related Information

Links

Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.
URLs http://www.opeal.com.cn/english/products_op06.htm
OP-6 Kaolin

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy