1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

NSC Kaolin

Oxide Analysis Formula Tolerance
CaO 0.05% -
K2O 2.10% 0.06
MgO 0.30% 0.02
Na2O 0.10% -
TiO2 0.04% -
Al2O3 37.00% 1.00
SiO2 48.00% 2.20
Fe2O3 0.80% 0.01
LOI 11.90%n/a
Oxide Weight 243.67
Formula Weight 276.58

Notes

Particle Size Distribution:
>53 microns: 0.05 max
>10 microns: 16
<2 microns: 40

Modulus of Rupture, Kgf/cm2:
At 80% Relative Humidity: 8.0
Dried at 110C: 16.2

Casting Rate @ 69% solids (mm2/min): 1.0
% P84 Deflocculant Required for 5 Poise Slip: 0.5

1180C 1280C
Fired Absorption: 16% 8%
Fired Shrinkage: 7% 11%
Brightness: 85 85

Related Information

Links

Minerals Mica
See Muscovite.
Minerals Kaolinite
The most fundamental clay mineral. This mineral is found in nature in its purest form as kaolin. How
Materials Grolleg Kaolin
A white burning kaolin from the UK, commonly used in porcelain bodies and as a glaze suspender. Sticky when wet, low plasticity.
Materials Standard Porcelain Kaolin
Materials Super Standard Porcelain
Materials Remblend Kaolin
Materials Treviscoe Kaolin
Materials English Kaolin
Materials Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries.
Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy