Quartz 762

Alternate Names: Kuvars 762

Oxide Analysis Formula Tolerance
CaO 0.14% 0.27
SiO2 98.60% 175.13
Al2O3 0.63% 0.66
TiO2 0.04% 0.05
Fe2O3 0.04% 0.03
MgO 0.15% 0.40
Na2O 0.09% 0.15
K2O 0.16% 0.18
LOI 0.15%n/a
Oxide Weight 10,658.90
Formula Weight 10,674.92

Notes

Available in -100, -63 and -45 micron sizes.

Related Information

Links

Materials Quartz 741
Materials Quartz 761
Typecodes Kaolin