Old Mine Kaolin

Description: Originally from Harris Mining Co.

Oxide Analysis Formula Tolerance
SiO2 45.72% 2.07
Al2O3 37.53% 1.00
Fe2O3 1.16% 0.02
TiO2 0.08% -
K2O 1.17% 0.03
Na2O 0.15% 0.01
LOI 14.04%n/a
Oxide Weight 233.22
Formula Weight 271.31

Related Information

Links

Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy