Ione kaolin

Oxide Analysis Formula Tolerance
CaO 0.10% 0.01
K2O 0.15% -
MgO 0.10% 0.01
Na2O 0.15% 0.01
TiO2 2.80% 0.10
Al2O3 34.40% 1.00
SiO2 48.60% 2.40
Fe2O3 0.60% 0.01
LOI 12.90%n/a
Oxide Weight 257.67
Formula Weight 295.83

Notes

Their data sheet describes it as "high-purity kaolin clay low in iron and alkali content processed for use as a raw material in the rubber, fiberglass, drywall, adhesives, ceramics, and agriculture industry."

Though not as high in purity as some of the other Kaolins Ione Kaolin is an economic source of low iron clay for applications where some impurities can be tolerated. It is a local central California clay, the only kaolin mined in the west of the continent.

Less that 1.5% > 325 mesh (47% minus 2 microns).

Related Information

Links

Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.
URLs https://usminecorp.com/wp-content/uploads/2020/09/Ione-Airfloated-Kaolin-K2Q-TDS-2020.pdf
Technical data sheet for Ione air floated kaolin
URLs https://usminecorp.com/
US Mine corporation website

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy